journal article·2017-03-04

Precipitation behaviour of oxide in directionally solidified aerospace bearing steel

F. Wang, L. Zheng, H. Zhang

Materials Science and Technology· Volume 33· Issue 4
Publisher page

Abstract

The directional solidification enables independently control of the holding temperature and withdrawal rate over a given range. This technology was used to investigate the precipitation behaviour of oxide in aerospace bearing steel M50NiL. Most of the oxides are Si–Al–Mn–Ti–O complex inclusions with spherical shape. With the increase of withdrawal rate, the size and volume fraction of oxides decrease. In contrast, the diameter and volume fraction increase remarkably with the increase of holding temperature. The composition of oxides with different sizes varies with holding temperature. The holding temperature of 1550°C accompanied with a cooling rate over 95.7°C min−1 is deemed as the optimal solidification parameters for M50NiL steel, which can significantly reduce the size and volume fraction of oxides.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering, Beihang University, Beijing 100191, People’s Republic of China

Funding

National High-Tech Program (863) of PR China

References (27)

Show source-provided references
1. 10.1007/s11837-012-0421-210.1007/s11837-012-0421-2 ↗
2. 10.1007/s11837-013-0687-z10.1007/s11837-013-0687-z ↗
3. 10.1007/s11661-012-1344-910.1007/s11661-012-1344-9 ↗
4. 10.1179/1743284713Y.000000049110.1179/1743284713Y.0000000491 ↗
5. 10.1007/s11837-013-0688-y10.1007/s11837-013-0688-y ↗
6. 10.2355/isijinternational.38.4610.2355/isijinternational.38.46 ↗
7. 10.1007/s11663-000-0077-010.1007/s11663-000-0077-0 ↗
8. 10.1016/S1005-0302(12)60110-810.1016/S1005-0302(12)60110-8 ↗
9. 10.1007/s11663-006-0057-010.1007/s11663-006-0057-0 ↗
10. 10.1016/S1359-6454(98)00388-710.1016/S1359-6454(98)00388-7 ↗
11. 10.1016/S1359-6454(01)00134-310.1016/S1359-6454(01)00134-3 ↗
12. 10.1016/S1359-6454(02)00560-810.1016/S1359-6454(02)00560-8 ↗
13. 10.1016/j.scriptamat.2005.08.00110.1016/j.scriptamat.2005.08.001 ↗
14. 10.2355/isijinternational.35.70810.2355/isijinternational.35.708 ↗
15. 10.2355/isijinternational.34.41410.2355/isijinternational.34.414 ↗
16. 10.1016/j.pmatsci.2011.06.00210.1016/j.pmatsci.2011.06.002 ↗
17. 10.1016/S1000-9361(07)60058-210.1016/S1000-9361(07)60058-2 ↗
18. M. A. Van Ende: ‘Formation and morphology of non-metallic inclusions in aluminium killed steels[D]’, 39–43; 2010, Louvain, Catholic University of Louvain.
19. Yanqing S. · J. Cryst. Growth · 2010 · 312 · 2441
20. 10.1016/j.msea.2006.07.02410.1016/j.msea.2006.07.024 ↗
21. 10.1179/03019230322500419610.1179/030192303225004196 ↗
22. 10.1179/03019230322500955110.1179/030192303225009551 ↗
23. 10.1016/j.jeurceramsoc.2012.11.00610.1016/j.jeurceramsoc.2012.11.006 ↗
24. 10.1016/j.scriptamat.2012.04.02510.1016/j.scriptamat.2012.04.025 ↗
25. 10.1016/j.msea.2006.08.03910.1016/j.msea.2006.08.039 ↗
26. 10.1016/j.scriptamat.2005.08.00110.1016/j.scriptamat.2005.08.001 ↗
27. 10.2355/isijinternational.38.4610.2355/isijinternational.38.46 ↗