Recovering high-purity silicon from mono-/poly-silicon cutting loss slurry

Yang Qi

Abstract

To improve the recovery of high purity silicon from cutting loss slurry,the sediment process and conditions are optimized.According to the physical and chemical character of mono-/poly-silicon cutting loss slurry,a system of water/polyethylene glycol=(8~9)∶1 with a few inorganic salt was introduced.The orthogonal tests were carried out with different sediment time and solid-to-liquid ratio,and the recycled silicon was purified by hydrochloric acid and hydrofluoric acid followed by ingot casting at 1500~1600℃.X-ray diffraction(XRD),X-ray fluorescence(XRF)and Particle size analyzer were adopted to investigate the influence of sediment condition on the recycled silicon.It is demonstrated that the Si and SiC content of the sample is respectively up to 88.52%and 11.46%under condition of solid-to-liquid ratio 0.06 and 5 h for sediment time.Silicon ingot purity reaches 98.71%after casting,and recovery ratio of Si achieves 43.33%.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.