journal article·2012-12

Self-welding susceptibility of cold worked alloy D9 and 316LN austenitic steels in flowing sodium

C Meikandamurthy, H Kumar, G Chakraborty, S K Albert, V Ramakrishnan, S Chandramouli, K K Rajan, A K Bhaduri

Materials Science and Technology· Volume 28· Issue 12
Publisher page

Abstract

Specimens of 20 cold worked alloy D9 and 316LN were tested for self-welding susceptibility in flowing sodium at 823 K. A contact stress of 24·5 MPa was maintained during the test, and tests were carried out for two different durations of 3 and 4·5 months for each. It was found that susceptibility to self-welding in flowing sodium is higher for cold worked alloy D9 than for cold worked 316LN. This is in contrast with no self-welding reported for annealed alloy D9 and high susceptibility to self-welding reported for annealed austenitic stainless steels like 316LN, 321 and 304. Dynamic recrystallisation of the cold worked structure at the location of self-welding, which does not occur for cold worked 316LN steel, is the reason attributed to the high susceptibility of cold worked alloy D9 to self-welding. It appears that carburisation of cold worked alloy surface, which leads to the formation of coarse TiC precipitates at the surfaces, assists dynamic recrystallisation.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Non-Destructive Testing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Fast Reactor Technology Group, Indira Gandhi Centre for Atomic Research, Kalpakkam 603102, India

Metallurgy & Materials Group, Indira Gandhi Centre for Atomic Research, Kalpakkam 603102, India

References (10)

Show source-provided references
1. 10.1016/0043-1648(93)90530-Y10.1016/0043-1648(93)90530-Y ↗
2. 10.13182/NT88-A1606110.13182/NT88-A16061 ↗
3. Huber F, Mattes K: ‘Investigations into self-welding behavior of metallic materials exposed to sodium’, Proc. Int. Conf. on ‘Liquid metals technology in energy production’, Champion, PA, USA, May 1976, 177–183.
4. Yoshida E, Hirakawa Y, Kano S, Nihei I: ‘In-sodium tribological study on colbalt-free hard facing materials for contact and sliding parts of FBR components’, Proc. Conf. on ‘Liquid metal engineering and technology’, Avignon, France, October 1988, Societe Francaise d'Energie Atomique Paris, 502-1–502-10.
5. Agostini P, Masetti E: ‘Friction tests of PEC reactor elements prototypic specimens with sodium and air’, Proc. Conf. on ‘Liquid metal engineering and technology’, Avignon, France, October 1988, Societe Francaise d'Energie Atomique Paris, 501-1–501-9.
6. 10.1016/j.jnucmat.2007.07.00310.1016/j.jnucmat.2007.07.003 ↗
7. 10.1504/IJNEST.2010.03347510.1504/IJNEST.2010.033475 ↗
8. 10.1016/j.jnucmat.2010.10.00210.1016/j.jnucmat.2010.10.002 ↗
9. 10.1016/0022-3115(92)90332-F10.1016/0022-3115(92)90332-F ↗
10. 10.1016/0022-3115(96)00377-710.1016/0022-3115(96)00377-7 ↗