Semisolid processing of short and long freezing range Cu alloys by electric current
Source abstract
Abstract
The present study reports the effect of ac (50 Hz) electric current treatment (ECT) on short freezing range (Cu–Ni) and long freezing range (Cu–Sn) alloys. This treatment was conducted during the semisolid state of the alloys, i.e. during casting in sand moulds. In isomorphous Cu–Ni alloy, with gradual increase in the electric current, first, the dendrites are refined; then, the refined dendrites are fragmented; and finally, the fragmented dendrites are refined. The ECT also reduces homogenisation treatment time. It is observed that a small amount of electric energy spent during sand casting saves considerable amount of energy for homogenisation treatment. The sand castings of Cu–Sn (peritectic) alloys are very much prone to interdendritic shrinkage. Thus, the density of castings is reduced. However, the ECT during casting increases the density of castings by reducing interdendritic shrinkage, modifies phase diagram of Cu–Sn alloy, increases volume fraction of the primary α phase (Cu) and reduces volume fraction of the peritectic phase. The ECT also refines the peritectic phase that transforms to δ phase on cooling to room temperature.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
National Metallurgical Laboratory CSIR, Jamshedpur 831007, India
References (29)
Show source-provided references
1. Spencer DB · PhD. Thesis, MIT, Cambridge, MA · 1971
2. Yurko JA, Martinez RA, Flemings MC: Metallurgical Science and Technology, 2003, 21, (1), 10–15.
3. 10.1007/BF0266109010.1007/BF02661090 ↗
4. Dutta P · Indian Foundry J. · 2009 · 55 · 33
5. ‘Bone frontier induction’, available at: http://www.bonefrontier.com/ssm.htm.
6. ‘Semi-solid casting’, available at: http://www.flow3d.com/apps/cast/app_cast_semi_1.html.
7. Barman N, Dutta P: ‘Studies on transport phenomena during rheocasting in presence of electromagnetic stirring’, availale at: http://mme.iitm.ac.in/icssp4/abstracts/nbarman.
8. Vforge Inc., available at: http://www.vforge.com.
9. Fan Z: Int. Mater. Reviews, 2002, 47, (2), 1–37.10.1179/095066001225001076 ↗
10. Wang H · Mater. Sci. Technol. · 2005 · 21 · 65
11. Kazakov AA · Adv. Mater. Process · 2000 · 157 · 31
12. ‘The metal casting’, available at: http://www.themetalcasting.com/articles/2008/08.
13. ‘Semi-solid metal casting’, available at: http://en.wikipedia.org/wiki/Semi-solid_metal_casting.
14. Industrial Materials Institute, available at: http://imi.cnrc-nrc.gc.ca/docs/factsheets/moulage-semi-solids-e.pdf.
15. ‘Electrohydrodynamics (EHD)’, available at: http://en.wikipedia.org/wiki/Electrohydrodynamics.
16. ‘Electrohydrodynamic multiphase flow’, available at: http://www.me.wpi.edu/Research/MFG/Research/.
17. Khan DC: Indian Institute of Technology, Kanpur, India, Personal communication, 2005.
18. Prodhan A: Indian Patent no.: 226266, 2008.
19. 10.1023/A:101856902847110.1023/A:1018569028471 ↗
20. 10.1007/s11663-001-0060-410.1007/s11663-001-0060-4 ↗
21. Prodhan A · AFS Trans. · 2008 · 08 · 233
22. Prodhan A · AFS Trans. · 2009 · 117 · 63
23. Maity PC: DAV Institute of Engineering and Technology, Kabirnagar, Jalandhar, Punjab, India, Personal communication, 2008.
24. Mondal D: National Metallurgical Laboratory, Jamshedpur, India, Personal communication, 2008.
25. Prodhan A · Indian Foundry J. · 2010 · 56 · 27
26. ‘The copper–nickel application’, available at: http://www.sv.vt.edu/classes/MSE2094_NoteBook/96ClassProj/examples/cuni.html.
27. Ordonez S · Int. J. Met. Cast. · 2009 · 3 · 37
28. Hanson D, Pellwalpole WT: ‘Chill cast tin bronzes’, 60; 1951, London, Edward Arnold & Co.
29. Chrianjeevi K · Indian Foundry J. · 2007 · 53 · 45