journal article·2013-12

Precipitate morphology and effects on strength of laser welded Mg–Nd–Zn–Zr after aging treatment

L Yang, J Dai, L L Li, G L Guo, L Z Guo, G L Zhao

Materials Science and Technology· Volume 29· Issue 12
Publisher page

Abstract

Magnesium rare earth alloys have been received extensive attention due to their attractive mechanical properties. The precipitation sequence in laser welded Mg–3Nd–0·2Zn–0·4Zr (NZ30K) alloy during aging treatment has been investigated using transmission electron microscopy (TEM). The results show that the tensile strength of laser welded NZ30K can be improved significantly after aging treatment at 200°C for 8 h. The precipitation in laser welded NZ30K alloy follows the sequence of super saturated solid solution→ β″(DO19)→ β′(fcc)→ β. The results of incremental of critical shear stress component are Δ τs/Δ τp/Δ τr/Δ τf = 1·86∶3·57∶3·14∶1. The platelet of precipitates with high volume fraction is the most important factor that enhances aging treatment strengthening.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Hydrogen Storage and Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Mechanical Engineering, Changshu Institute of Technology, Changshu 215500, China

School of Materials Science and Engineering, China University of Mining and Technology, Xuzhou 221116, China

China Gridcom Company, LTD, Beijing 100070, China

References (23)

Show source-provided references
1. 10.1179/026708309X1250693387370110.1179/026708309X12506933873701 ↗
2. 10.1179/1743284712Y.000000006510.1179/1743284712Y.0000000065 ↗
3. 10.1016/j.matdes.2009.08.04010.1016/j.matdes.2009.08.040 ↗
4. 10.1179/026708310X1266841553388310.1179/026708310X12668415533883 ↗
5. 10.1007/s10853-012-6408-010.1007/s10853-012-6408-0 ↗
6. 10.1016/S1003-6326(07)60242-810.1016/S1003-6326(07)60242-8 ↗
7. 10.1179/1743284712Y.000000008410.1179/1743284712Y.0000000084 ↗
8. 10.1179/174328409X40757910.1179/174328409X407579 ↗
9. 10.1007/s10800-007-9426-x10.1007/s10800-007-9426-x ↗
10. Fu PH · Mater. Sci. Eng. A · 2008 · 486 · 18310.1016/j.msea.2007.08.064 ↗
11. 10.1016/j.electacta.2006.09.06910.1016/j.electacta.2006.09.069 ↗
12. 10.1016/j.corsci.2006.12.01110.1016/j.corsci.2006.12.011 ↗
13. 10.1016/j.actamat.2011.03.03810.1016/j.actamat.2011.03.038 ↗
14. 10.1016/j.actamat.2009.06.00310.1016/j.actamat.2009.06.003 ↗
15. 10.1016/S0968-4328(00)00094-910.1016/S0968-4328(00)00094-9 ↗
16. Karimzadeh H, Worrall JM, Pilkington R, Lorimer GW: ‘Magnesium technology’, Proc. Conference, 1st edn, 138–141; London, 1986.
17. 10.1016/S0921-5093(01)01291-610.1016/S0921-5093(01)01291-6 ↗
18. Atiya G · Magnes. Technol · 2011 · 249
19. Villars P · Metals Park, OH, American Society for Metals · 1985 · 3 · 2710
20. 10.1016/j.jallcom.2005.11.04610.1016/j.jallcom.2005.11.046 ↗
21. 10.1016/S1359-6454(03)00391-410.1016/S1359-6454(03)00391-4 ↗
22. He SM: ‘Study on the microstructural evolution, properties and fracture behavior of Mg-Gd-Y-Zr(-Ca) alloys’, PhD thesis, Shanghai Jiao Tong University, Shanghai, China, 2007, 219–222.
23. 10.1016/S1359-6462(02)00497-910.1016/S1359-6462(02)00497-9 ↗