Stepped heat treatment for austempering of high manganese alloyed ductile iron
Source abstract
Abstract
A stepped heat treatment is proposed for overcoming the difficulty of obtaining ductility in an austempered alloyed ductile iron. The method is illustratedfor an iron containing 0·67%Mn, 0·25%Mo, and 0·25%Cu, using an austenitising temperature of 920°C, afirst step austempering temperature of 400°C for 120 min, and a second step austempering temperature of 285°C. The change in the microstructure and phase characteristics with time during the second austempering step are described. Related changes in the mechanical properties compared with a single austempering treatment at 400°C are an increase in the ultimate tensile strength from 770 to 970 MN m−2, an increase in elongation from 2·5 to 7·5%, and an increase in the unnotched Charpy impact energy from 40 to 150 J.MST/3119
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Metallurgy and Material Forming · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. 1993 · 9 · 572
2. 1993 · 9 · 586
3. 1993 · 9 · 882
4. 1994 · 10 · 3510.1179/mst.1994.10.1.35 ↗
5. 1994 · 10 · 105010.1179/mst.1994.10.12.1050 ↗
6. 1995 · 11 · 11810.1179/mst.1995.11.2.118 ↗
7. 1995 · 11 · 77610.1179/mst.1995.11.8.776 ↗
8. 1995 · 11 · 90810.1179/mst.1995.11.9.908 ↗
9. 1994 · 10 · 106810.1179/mst.1994.10.12.1068 ↗