Source abstract
Abstract
Measurements of the average austenite carbon content, retained austenite content, unreacted austenite content, and mechanical properties are reportedfor various austempering heat treatments of an alloyed ductile iron of composition (wt-%) Fe-3.39C-2.56Si-0.37Mn-0.25Mo-0.29Cu-0.04Mg. It is shown that a stepped austempering treatment can be used to considerably increase the ductility of the alloy compared with a single heat treatment and to extend the austempering time interval over which the ASTM standard can be satisfied. Decreasing the second step austempering temperature accelerates the stage I reaction during the second step treatment but produces little change in the mechanical properties of the alloy used in the present work. Decreasing the first step austempering time to 375°C accelerates the stage I reaction in the second step treatment but slightly decreases the maximum impact energy and increases the austempering time at which it is achieved.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Metallurgy and Material Forming · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. 1995 · 11 · 908
2. 1995 · 11 · 776
3. 1995 · 11 · 293
4. 1995 · 11 · 118
5. 10.1179/02670830112500018610.1179/026708301125000186 ↗
6. 1993 · 9 · 88210.1179/mst.1993.9.10.882 ↗
7. 1993 · 9 · 586
8. 1993 · 9 · 572
9. 1997 · 13 · 11710.1179/mst.1997.13.2.117 ↗
10. 1995 · 11 · 1007
11. 1994 · 10 · 106810.1179/mst.1994.10.12.1068 ↗
12. 1997 · 13 · 2410.1179/mst.1997.13.1.24 ↗