Abstract
316L-30W composites were successfully fabricated via spark plasma sintering at 1550°C to evaluate their potential as the interlayer between W and 316L stainless steel in fusion reactors. The effect of holding time on the microstructure and its subsequent effects on the fracture morphology and wear properties of the composites were investigated. The results show that more W particles melted and reacted with 316L steel as the holding time increased from 1 to 5 min. The generation of voids was mainly caused by the differences in diffusivity and the coefficient of thermal expansion between W and 316L. The 316L-30W composite held for 3 min had a smaller and more stable friction coefficient, indicating that its interface was firmly bonded and homogeneous. This paper is part of a thematic issue on Nuclear Materials.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Fusion materials and technologies · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Chongqing Institute of Green and Intelligent Technology, Chinese Academy of Sciences, Chongqing, People's Republic of China
College of Materials Science and Engineering, Chongqing University, Chongqing, People's Republic of China
Chongqing Key Laboratory of Additive Manufacturing Technology and Systems, Chongqing, People's Republic of China
Funding
Key Deployment Projects of Chinese Academy of Sciences · Ministry of Education of China.
References (29)
Show source-provided references
1. 10.1088/0031-8949/2014/T159/01400610.1088/0031-8949/2014/T159/014006 ↗
2. 10.1016/j.jnucmat.2013.02.07410.1016/j.jnucmat.2013.02.074 ↗
3. 10.1016/j.jnucmat.2012.08.01810.1016/j.jnucmat.2012.08.018 ↗
4. 10.1016/B978-0-08-056033-5.00019-710.1016/B978-0-08-056033-5.00019-7 ↗
5. 10.1016/j.jnucmat.2007.03.22210.1016/j.jnucmat.2007.03.222 ↗
6. 10.1016/j.fusengdes.2014.01.02810.1016/j.fusengdes.2014.01.028 ↗
7. 10.1016/j.ijrmhm.2014.09.00210.1016/j.ijrmhm.2014.09.002 ↗
8. 10.1016/j.jallcom.2009.09.10510.1016/j.jallcom.2009.09.105 ↗
9. 10.1016/j.fusengdes.2014.02.06310.1016/j.fusengdes.2014.02.063 ↗
10. 10.1016/j.fusengdes.2015.06.15410.1016/j.fusengdes.2015.06.154 ↗
11. 10.1088/0031-8949/2014/T159/01403410.1088/0031-8949/2014/T159/014034 ↗
12. 10.1016/j.fusengdes.2005.07.01510.1016/j.fusengdes.2005.07.015 ↗
13. 10.1016/j.jnucmat.2015.11.02410.1016/j.jnucmat.2015.11.024 ↗
14. 10.1016/j.fusengdes.2017.08.00110.1016/j.fusengdes.2017.08.001 ↗
15. 10.1016/j.jnucmat.2015.10.04510.1016/j.jnucmat.2015.10.045 ↗
16. Figiel P · Arch Mater Sci Eng · 2008 · 33 · 83
17. 10.1179/174329008X29373210.1179/174329008X293732 ↗
18. Nagender N · J Alloy Phase Diag · 1986 · 2 · 176
19. 10.1016/j.matdes.2016.01.04210.1016/j.matdes.2016.01.042 ↗
20. 10.1016/S0921-5093(00)01989-410.1016/S0921-5093(00)01989-4 ↗
21. 10.1016/j.compscitech.2005.05.02710.1016/j.compscitech.2005.05.027 ↗
22. 10.1007/BF0274977110.1007/BF02749771 ↗
23. 10.1016/j.matdes.2011.04.03210.1016/j.matdes.2011.04.032 ↗
24. 10.1016/j.msea.2017.02.04910.1016/j.msea.2017.02.049 ↗
25. 10.1016/j.jnucmat.2014.07.01110.1016/j.jnucmat.2014.07.011 ↗
26. 10.1016/j.jallcom.2008.05.06810.1016/j.jallcom.2008.05.068 ↗
27. 10.1016/j.apsusc.2017.03.26310.1016/j.apsusc.2017.03.263 ↗
28. 10.1016/j.jallcom.2017.04.10410.1016/j.jallcom.2017.04.104 ↗
29. 10.1016/j.wear.2010.09.00110.1016/j.wear.2010.09.001 ↗