Effects of initial undercooling on microstructure formation and recrystallisation of undercooled melts
Source abstract
Abstract
The critical undercoolings for the two grain refinement events and the onset of recrystallisation event are determined by detailed analysis of the microstructure evolution of bulk undercooled Ni–20 at.-%Cu alloy melts. The first grain refinement event occurred in the low undercooling range was explained by dendrite remelting. The second grain refinement event occurred in the high undercooling range was due to the combined effects of dendrite remelting stress-induced dendrite breakup during recalescence and recrystallisation during the near-equilibrium solidification stage after recalescence. The micro-stress induced by the solidification contraction during recalescence in the so called ‘first mushy zone’ would lead to distortion and breakup of primary dendrites. The stress-induced broken-up dendrites have sufficient driving force for recrystallisation.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Solidification and crystal growth phenomena · Metallic Glasses and Amorphous Alloys · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
College of Materials Science and Engineering, North University of China, Taiyuan, PR China
State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an, PR China
Funding
Ministry of Science and Technology of the People's Republic of China · National Natural Science Foundation of China · Shanxi Scholarship Council of China
References (21)
Show source-provided references
1. Walker JL. · The physical chemistry of process metallurgy, Part 2 · 1959
2. 10.1016/0001-6160(65)90033-710.1016/0001-6160(65)90033-7 ↗
3. 10.1016/0017-9310(65)90110-910.1016/0017-9310(65)90110-9 ↗
4. Jackson KA · J Mater Sci Lett. · 1969 · 245 · 407
5. 10.1007/BF0072326510.1007/BF00723265 ↗
6. 10.1016/0927-796X(94)90011-610.1016/0927-796X(94)90011-6 ↗
7. 10.1179/174328006X10248410.1179/174328006X102484 ↗
8. 10.1016/S0921-5093(01)00929-710.1016/S0921-5093(01)00929-7 ↗
9. 10.1016/S0022-0248(01)01438-510.1016/S0022-0248(01)01438-5 ↗
10. Karma A. · Int J Non-Equilibrium Proc. · 1998 · 11 · 201
11. 10.1016/S0022-0248(98)00399-610.1016/S0022-0248(98)00399-6 ↗
12. Christian JW. · 2002
13. Boettinger W · 1988
14. Piccone TJ · Metall Trans A · 1987 · 18 · 92510.1007/BF02646934 ↗
15. 10.1016/j.jcrysgro.2007.09.00510.1016/j.jcrysgro.2007.09.005 ↗
16. 10.1016/j.matlet.2012.04.04210.1016/j.matlet.2012.04.042 ↗
17. 10.1016/j.jallcom.2007.04.03010.1016/j.jallcom.2007.04.030 ↗
18. 10.1063/1.11775510.1063/1.117755 ↗
19. 10.1007/s11663-999-0058-x10.1007/s11663-999-0058-x ↗
20. 10.1007/s10853-010-5189-610.1007/s10853-010-5189-6 ↗
21. 10.1016/j.jcrysgro.2016.09.01610.1016/j.jcrysgro.2016.09.016 ↗