Activation energy, viscosity and fragility of Cu–Zr–Ti–In bulk metallic glasses
Source abstract
Abstract
In the present paper, activation energy, viscosity and fragility of two In alloyed Cu–Zr–Ti–In bulk metallic glasses are evaluated by differential scanning calorimetry and thermomechanical analysis respectively. Eg of 60Cu–34Zr–5Ti–1In and 58Cu–34Zr–5Ti–3In is 175±9 and 182±5 kJ mol−1 respectively. Ex of 60Cu–34Zr–5Ti–1In and 58Cu–34Zr–5Ti–3In is 369±24 and 317±10 kJ mol−1 respectively, indicating that increasing the content of indium decreases the value of Ex of the as cast bulk metallic glasses. By means of comparison of activation energies referring to the crystallisation peak temperature, one can find that the second step crystallisation of both bulk metallic glasses is easier to occur. The possible phases of the annealed samples are determined. Thermomechanical analysis shows that viscosity for 58Cu–34Zr–5Ti–3In is larger than that for 60Cu–34Zr–5Ti–1In in the supercooled region, but Vogel–Fulcher–Tammann (VFT) temperature of 58Cu–34Zr–5Ti–3In is lower than that of 60Cu–34Zr–5Ti–1In. Both 60Cu–34Zr–5Ti–1In and 58Cu–34Zr–5Ti–3In bulk metallic glasses are stronger than o-terphenyl, but more fragile than SiO2. 58Cu–34Zr–5Ti–3In is stronger than 60Cu–34Zr–5Ti–1In. It indicates that increasing indium content can decrease the VFT temperature but make glass stronger.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Material Dynamics and Properties · Glass properties and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering, Jiangsu Key Laboratory for Advanced Metallic materials, Southeast University, Nanjing 211189, China
School of Materials Engineering, Nanjing Institution of Technology, Nanjing 211167, China
References (34)
Show source-provided references
1. 10.1016/S1359-6454(02)00024-110.1016/S1359-6454(02)00024-1 ↗
2. 10.1016/j.actamat.2006.04.00510.1016/j.actamat.2006.04.005 ↗
3. 10.1016/j.actamat.2004.02.00910.1016/j.actamat.2004.02.009 ↗
4. 10.1016/j.actamat.2003.12.00810.1016/j.actamat.2003.12.008 ↗
5. 10.1038/nmat98210.1038/nmat982 ↗
6. 10.1016/j.actamat.2011.01.02910.1016/j.actamat.2011.01.029 ↗
7. 10.1016/S1359-6454(01)00181-110.1016/S1359-6454(01)00181-1 ↗
8. 10.1016/j.actamat.2005.04.03710.1016/j.actamat.2005.04.037 ↗
9. 10.1016/j.actamat.2010.05.02610.1016/j.actamat.2010.05.026 ↗
10. 10.1016/j.actamat.2009.07.04210.1016/j.actamat.2009.07.042 ↗
11. 10.1016/j.pmatsci.2006.07.00310.1016/j.pmatsci.2006.07.003 ↗
12. 10.1016/j.msea.2006.02.24410.1016/j.msea.2006.02.244 ↗
13. 10.1007/s00339-012-6876-810.1007/s00339-012-6876-8 ↗
14. 10.1063/1.370072110.1063/1.3700721 ↗
15. Inoue A., and Zhang T. ‘Novel superplasticity of supercooled liquid for bulk amorphous alloys’, in ‘Superplasticity in Advanced Materials – Icsam-97’, (ed. Chokshi A. H.), 197–205; 1997, Zurich-Uetikon, Transtec Publications Ltd.
16. 10.1016/j.cplett.2007.06.03110.1016/j.cplett.2007.06.031 ↗
17. 10.1063/1.149951010.1063/1.1499510 ↗
18. 10.1007/3-540-30437-1_410.1007/3-540-30437-1_4 ↗
19. 10.1016/S0079-6425(00)00021-910.1016/S0079-6425(00)00021-9 ↗
20. 10.1016/j.jallcom.2005.07.06210.1016/j.jallcom.2005.07.062 ↗
21. 10.1016/j.jallcom.2006.08.34010.1016/j.jallcom.2006.08.340 ↗
22. 10.1021/ac60131a04510.1021/ac60131a045 ↗
23. 10.1016/S0925-8388(01)01977-610.1016/S0925-8388(01)01977-6 ↗
24. 10.1063/1.11489110.1063/1.114891 ↗
25. 10.1063/1.292745910.1063/1.2927459 ↗
26. 10.1063/1.345767010.1063/1.3457670 ↗
27. 10.1111/j.1151-2916.1925.tb16731.x10.1111/j.1151-2916.1925.tb16731.x ↗
28. 10.1016/j.intermet.2009.08.01510.1016/j.intermet.2009.08.015 ↗
29. 10.1063/1.46611710.1063/1.466117 ↗
30. 10.1016/0022-3093(85)90334-510.1016/0022-3093(85)90334-5 ↗
31. 10.1063/1.275926610.1063/1.2759266 ↗
32. 10.1063/1.350690010.1063/1.3506900 ↗
33. 10.1103/PhysRevB.74.06420310.1103/PhysRevB.74.064203 ↗
34. 10.1103/PhysRevB.76.10420210.1103/PhysRevB.76.104202 ↗