Abstract

The microstructure of Fe 3 Al/18-8 diffusion bonding joint after heat treatment was analysed by metalloscopy, scanning electron microscopy and X-ray diffraction. The experimental results indicated that the size of grains near the Fe 3 Al/18-8 diffusion interface was decreased significantly and the microstructure near the interface became homogeneous. The precipitations also became tiny with regular shape and were distributed evenly at the interface region. The microhardness of the Fe 3 A1/18-8 diffusion bonding joint was decreased and no brittle phase with high microhardness existed near the interface after heat treatment. The suitable parameters of heat treatment were: heating temperature T =800°C, holding time t =30 min, furnace cooling to 700°C then air cooling.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Advanced Welding Techniques Analysis · Semiconductor materials and interfaces

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (8)

Show source-provided references
1. 10.1557/JMR.1991.177910.1557/JMR.1991.1779 ↗
2. Yoo M. H.: J. Intermetallic. 1998 6 (7/8) 597.10.1016/S0966-9795(98)00033-8 ↗
3. 10.1016/S1359-6462(01)01142-310.1016/S1359-6462(01)01142-3 ↗
4. Li Y. J., , Wu H. Q., , Wang J., and Yin Y. S.: Mater. Sci Technol, 2003, 19, (2), 227.
5. 10.1007/BF0270801110.1007/BF02708011 ↗
6. David S. A. and Zacharia T.: Weld. 1 1993 5 (72) 201.10.2307/20045655 ↗
7. 10.3901/JME.2000.08.05510.3901/JME.2000.08.055 ↗
8. Wang J. Li Y. J. and Liu P.: Mater. Lett. 2003 57 (26/27) 4323.10.1016/S0167-577X(03)00311-2 ↗