journal article·2008-06

Hydrogen induced cracking and pitting of brass heat exchanger tube

Amjad Saleh El-Amoush

Materials Science and Technology· Volume 24· Issue 6
Publisher page

Abstract

Tin brass heat exchanger tube specimens were precharged with hydrogen at different cathodic charging conditions. Cathodic hydrogen charging was found to induce severe cracking and blistering on the surface of brass heat exchanger tube without externally applied stress. Microscopic observations revealed that the hydrogen cracks were intergranular (IG) or transgranular (TG) or mixed mode of cracking, i.e. IG and TG, while the blisters were observed to be spherically shaped. The severity of hydrogen induced cracking and blistering increased with the cathodic current density. Free corrosion immersion experiments were conducted on the hydrogen precharged tin brass heat exchanger tube specimens in 0·5M NaCl solution to investigate the role of hydrogen in pitting corrosion. It was found that hydrogen significantly promoted pit initiation and pit growth. Moreover, the pit formation and growth increased with charging time. The corrosion potential measurements revealed that the hydrogen precharged tin brass heat exchanger tube specimens exhibited lower corrosion resistance as compared with the non-precharged specimen. The corrosion potential of hydrogen precharged specimens reached a steady state after a longer immersion time. Furthermore, with increasing precharging time, the immersion time required to reach a steady state potential increased.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Vaughan H. G. · Weld · 1952 · 1 · 40
2. 10.1016/0001-6160(63)90214-110.1016/0001-6160(63)90214-1 ↗
3. Tetelman A. S.: Proc. Conf. on ‘Fundamental aspects of stress corrosion cracking’, 446; 1969, Houston, TX, National Association of Corrosion Engineers.
4. Bernstein I. M.: Metall Trans. 1970, 1, 3143.10.1007/BF03038430 ↗
5. Smialowski S.: in ‘Stress corrosion cracking and hydrogen embrittlement of iron base alloys’, (ed. Staele R. W. et al),405; 1973, Houston, TX, National Association of Corrosion Engineers.
6. Dos K. B., Roberts E. C., and Bassett R. G.: in ‘Hydrogen in metals’ (Proc. Int. Conf. on ‘Effects of hydrogen on materials properties and selection of structural design’), (ed.Bernstein I. M., and Thompson A. W.), 289; 1973, Metals Park, OH, ASM.
7. 10.1016/0010-938X(93)90190-R10.1016/0010-938X(93)90190-R ↗
8. Lynch S. P.: Acta Metall. 1984, 32, 79.10.1016/0001-6160(84)90204-9 ↗
9. Smialwski M. ‘Hydrogen in steel’, 1926, Oxford, Pergamon.
10. Kerns G. E. · Scr. Metall · 1972 · 6 · 2107
11. Lynch S. P. · Met. Forum · 1979 · 2 · 189
12. Louthan M. R., and McNiff R. P. in ‘Effect of hydrogen on behavior of materials’, (ed.Thompson A. W., and Bernstein I. M.), 496; 1976, New York, TMS-AIME.
13. Birnbaum K. H. ‘Environment-sensitive fracture of engineering materials’, (ed.Foroulis Z. A.), 327-359; 1979, Warrendale, PA, The Metallurgical Society of AIME.
14. 10.5006/1.328485410.5006/1.3284854 ↗
15. 10.5006/0010-9312-36.2.6710.5006/0010-9312-36.2.67 ↗
16. 10.5006/0010-9312-30.2.4710.5006/0010-9312-30.2.47 ↗
17. Kimura A. · Scr. Metall · 1988 · 36 · 757
18. 10.1007/BF0266960810.1007/BF02669608 ↗
19. 10.1080/1478644120856113110.1080/14786441208561131 ↗