Abstract

The microstructure and internal friction of Ni–Ti alloys after hydrogen absorption have been investigated by means of optical microscopy, X-ray diffraction, differential scanning calorimetry and low frequency torsional internal friction apparatus. The results show that, after hydrogen absorption, the grains tend to be elongated, and the nucleation and growth of hydrides are mainly concentrated at the grain boundaries. In addition, a new phase ultimately identified as Ti2NiH0·5 phase forms after absorption of hydrogen. The hydrogen induced martensite promotes the emergence of a two-stage transformation. However, the growth of hydrides causes a reduction of the hydrogen induced martensite. The hydrides act as strong pinning points, resulting in a dramatic increase in the internal friction. In addition, the marked change of the internal stress, caused by the microscopic strain and the mismatching of the volumes, also improves the internal friction.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen Storage and Materials · Intermetallics and Advanced Alloy Properties · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

College of Materials Science and Engineering Nanjing University of Technology, Nanjing 210009, China

BASF-YPC Company Limited Nanjing 210048, China

References (12)

Show source-provided references
1. 10.1016/0925-8388(93)90582-810.1016/0925-8388(93)90582-8 ↗
2. 10.1016/S1359-6462(02)00099-410.1016/S1359-6462(02)00099-4 ↗
3. 10.2320/matertrans.43.79810.2320/matertrans.43.798 ↗
4. Wu JH · Rare Met. · 2005 · 24 · 190
5. 10.1016/S1359-6454(99)00337-710.1016/S1359-6454(99)00337-7 ↗
6. 10.1016/j.jallcom.2010.10.12810.1016/j.jallcom.2010.10.128 ↗
7. 10.1016/j.jallcom.2003.09.13510.1016/j.jallcom.2003.09.135 ↗
8. 10.1016/j.jallcom.2006.08.26810.1016/j.jallcom.2006.08.268 ↗
9. 10.1016/S0079-6425(99)00010-910.1016/S0079-6425(99)00010-9 ↗
10. 10.1016/S1359-6462(00)00672-210.1016/S1359-6462(00)00672-2 ↗
11. He JY · J. Mech. Strength · 2004 · 26 · 081
12. 10.1016/0925-8388(93)90582-810.1016/0925-8388(93)90582-8 ↗