journal article·2008-06

Investigation of interfacial reaction between eutectic Sn–Pb solder droplet and Au/Ni/Cu pad

F. Q. Li, C. Q. Wang, Y. H. Tian

Materials Science and Technology· Volume 24· Issue 6
Publisher page

Abstract

The basic process of molten droplet solder bumping and interfacial reaction between molten Sn–Pb droplet and Au/Ni/Cu under bump metallurgy (UBM) pad was investigated in the present paper. The morphology of intermetallic compounds was strongly influenced by the initial temperature of the solder droplet. When the initial temperature 350°C was reached, a continuous AuSn2 and needle like AuSn4 were formed at the solder bump/pad interface. When the initial temperature 450°C was reached, all the AuSn2 converted into AuSn4. Rod like AuSn4 grew strongly, some acicular AuSn4 was distributed inside the solder near the interface. Under the condition that the substrate was preheated, interfacial reaction is more intensive at the molten stage. Results of the calculation have shown that compared with the initial height of droplet, the contact temperature is mainly dependent on the initial temperature. To elucidate intermetallic formation mechanism at the interface, the pad/solder temperature field was analysed using finite element method (FEM).
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Nanomaterials and Printing Technologies · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Patterson D. S. · Adv. Electron. Pack · 1997 · 1 · 337
2. 10.1016/S0026-2714(99)00237-110.1016/S0026-2714(99)00237-1 ↗
3. Hotchkiss G., Amador G., Jacobs L., Stierman R., Dunford S., Hundt P., Beikmohamadi A., Cairncross A., Gantzhorn J., Quinn B., and Saltzberg M.: Proc. 48th Conf. on ‘Electronic components and technology’, Seattle, WA, May 1998, IEEE, 434.441.
4. 10.1109/6144.84678110.1109/6144.846781 ↗
5. 10.1109/6104.87324310.1109/6104.873243 ↗
6. 10.1016/S0924-0136(01)00740-310.1016/S0924-0136(01)00740-3 ↗
7. 10.1142/S096031319800019710.1142/S0960313198000197 ↗
8. 10.1016/S0927-796X(01)00029-810.1016/S0927-796X(01)00029-8 ↗
9. Bradley E. · IEEE. Trans. Comp. Pkg. Mfg. Technol. B · 1996 · 19 · 320
10. 10.1109/33.6257410.1109/33.62574 ↗
11. 10.1007/s11664-999-0162-310.1007/s11664-999-0162-3 ↗
12. 10.1007/s11664-000-0010-y10.1007/s11664-000-0010-y ↗
13. 10.1016/S0254-0584(97)02076-210.1016/S0254-0584(97)02076-2 ↗
14. 10.1063/1.36333610.1063/1.363336 ↗
15. 10.1016/S0017-9310(02)00289-210.1016/S0017-9310(02)00289-2 ↗
16. Geiger G. H., and Poirier D. R. ‘Transport phenomena in metallurgy’; 1996, Reading, MA, Addison-Wesley.
17. Lau J. H. ‘Ball grid array technology’, 205; 1995, New York, McGraw-Hill.
18. Rohsenow W. M. ‘Handbook of heat transfer fundamentals’, 2nd edn; 1985, New York, McGraw-Hill.
19. Bader W. G. · Weld. J · 1969 · 48 · 551s