Investigation of the microstructure and toughness of 550 MPa grade pipeline after the hot-bending process
Source abstract
Abstract
In this work, the effects of the hot-bending process on the microstructure and low temperature (−40°C) toughness of weld metal of pipeline K65 (the highest grade of the Russian natural gas pipeline) were studied. The weld metal from the longitudinally submerged arc welding (LSAW) pipe making process was compared with that subsequently treated by the hot-bending process. It was found that the latter process led to serious deterioration in toughness, which obviously degraded the sound properties achieved in the original weld metal of LSAW pipes. Microstructural characterisation revealed that the weld metal, which originally consisted mainly of acicular ferrite in the as-deposited condition, became predominantly composed of bainitic ferrite after hot bending. It is clear that reaustenisation caused a smaller austenite grain-sized matrix, which brought about a very high volume fraction of bainite. Consequently, the low temperature toughness was deteriorated, in contrast to the excellent toughness achieved in the as-deposited weld metal.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Materials Science and Engineering, University of Science and Technology, Beijing, China
Department of Materials Science and Engineering, National Taiwan University, Taipei, Taiwan
Institute of Research of Iron and Steel, Shasteel, Zhangjiagang, Jiangsu, China
CNPC Bohai Equipment Steel Pipe Research Institute, Qingxian, Hebei, China
References (50)
Show source-provided references
1. 10.1016/j.matchar.2011.05.01310.1016/j.matchar.2011.05.013 ↗
2. Shang C. J., Xia D. X., Wang X. L., Li X. C., and Nie W. J. ‘The development of third-generation pipeline steel in China’, 6th Int. Pipeline Technology Conference, Ostend, Belgium, 2013, 1–14.
3. 10.1007/s11661-015-2790-y10.1007/s11661-015-2790-y ↗
4. 10.1007/s11661-005-0315-910.1007/s11661-005-0315-9 ↗
5. Yang W. W. · Welded Pipe and Tube · 2013 · 36 · 67
6. 10.1002/9781119027973.ch8810.1002/9781119027973.ch88 ↗
7. 10.1016/j.msea.2006.12.09710.1016/j.msea.2006.12.097 ↗
8. 10.1016/j.msea.2007.06.03510.1016/j.msea.2007.06.035 ↗
9. 10.1007/s11661-009-0135-410.1007/s11661-009-0135-4 ↗
10. 10.1016/0921-5093(92)90361-410.1016/0921-5093(92)90361-4 ↗
11. 10.1016/0921-5093(92)90095-I10.1016/0921-5093(92)90095-I ↗
12. 10.2320/matertrans1989.34.65810.2320/matertrans1989.34.658 ↗
13. 10.2355/isijinternational.35.101310.2355/isijinternational.35.1013 ↗
14. 10.1016/S0254-0584(00)00379-510.1016/S0254-0584(00)00379-5 ↗
15. Zhang Z. · Weld. J. · 1997 · 76 · 183s
16. Wang W. · Weld. J. · 2002 · 81 · 132s
17. Keehan E. · Weld. J. · 2006 · 85 · 200s
18. Keehan E. · Weld. J. · 2006 · 85 · 218S
19. 10.1179/136217110X1266504820769210.1179/136217110X12665048207692 ↗
20. 10.1007/BF0113332710.1007/BF01133327 ↗
21. 10.1007/BF0120349810.1007/BF01203498 ↗
22. 10.1016/j.cossms.2004.10.00110.1016/j.cossms.2004.10.001 ↗
23. 10.1007/BF0058832510.1007/BF00588325 ↗
24. 10.1007/s11661-003-0010-710.1007/s11661-003-0010-7 ↗
25. 10.1179/1743284710Y.000000004710.1179/1743284710Y.0000000047 ↗
26. 10.1179/02670830077300263610.1179/026708300773002636 ↗
27. 10.1016/j.matdes.2015.09.07310.1016/j.matdes.2015.09.073 ↗
28. 10.1016/S1359-6454(02)00560-810.1016/S1359-6454(02)00560-8 ↗
29. 10.1179/1362171812Y.000000007110.1179/1362171812Y.0000000071 ↗
30. 10.1007/s12540-014-1013-110.1007/s12540-014-1013-1 ↗
31. 10.1179/174329306X12086810.1179/174329306X120868 ↗
32. 10.1179/026708310X1270114976805210.1179/026708310X12701149768052 ↗
33. 10.1179/174329306X11329910.1179/174329306X113299 ↗
34. 10.2355/isijinternational.54.93210.2355/isijinternational.54.932 ↗
35. 10.1016/j.msea.2011.10.01710.1016/j.msea.2011.10.017 ↗
36. 10.1016/j.msea.2014.07.10110.1016/j.msea.2014.07.101 ↗
37. 10.2355/isijinternational1966.26.41810.2355/isijinternational1966.26.418 ↗
38. Muthmann E. · Int. Symp. on ‘Microalloyed steels for the oil & gas industry’, Araxá, Brazil · 2006 · 1
39. 10.1016/S1006-706X(06)60090-310.1016/S1006-706X(06)60090-3 ↗
40. Shohei K. · JFE Tech. Rep. · 2015 · 20 · 106
41. Bajcer B. · Metalurgija · 2007 · 46 · 47
42. 10.1016/0026-0800(79)90041-710.1016/0026-0800(79)90041-7 ↗
43. 10.1016/S1359-6462(98)00170-510.1016/S1359-6462(98)00170-5 ↗
44. 10.1007/BF0264639610.1007/BF02646396 ↗
45. 10.1007/BF0073085910.1007/BF00730859 ↗
46. 10.1016/S1359-6462(00)00386-910.1016/S1359-6462(00)00386-9 ↗
47. 10.1007/s11661-004-1007-610.1007/s11661-004-1007-6 ↗
48. 10.1007/BF0267256710.1007/BF02672567 ↗
49. 10.1007/BF0050634110.1007/BF00506341 ↗
50. 10.1016/j.msea.2011.09.01710.1016/j.msea.2011.09.017 ↗