Abstract

In the present study, we carried out a flux cored arc welding using a super duplex stainless steel as a filler metal and analysed the cause of cracking that occurred at the aging treatment for 30 min at 850°C. The stress concentration effect by the notch of the welding bead affected the hot cracking susceptibility, and the impact value of weldment was remarkably decreased due to the precipitation of secondary phases. In addition, the precipitation of σ of the adjacent area to the crack was measured to be higher by ∼12 wt- than the non-adjacent area to the crack. As a result of analysis of fracture plane, it was embrittled by segregation of impurities or inclusions, which acted as a starting point of the crack, and the crack grew according to the widely distributed σ phase.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Materials Science and Engineering, Dong-A University, 840 Hadan-dong, Saha-gu, Busan 604-714, Korea

References (20)

Show source-provided references
1. 10.1016/S1044-5803(97)00144-710.1016/S1044-5803(97)00144-7 ↗
2. Lippold J. C., and Kotecki D. J. ‘Welding metallurgy and weldability of stainless steels’, 1st edn, 230; 2005, Hoboken, NJ, John Wiley & Sons.
3. 10.5006/1.358531210.5006/1.3585312 ↗
4. 10.1533/978184569877510.1533/9781845698775 ↗
5. Charles J.: Proc. 4th Int. Conf. on ‘Structure and mechanical properties of duplex stainless steel’, Glasgow, Scotland, November 1994, The Welding Institute (TWI), Paper KV.
6. Nicholls J. M.: Proc. 4th Int. Conf. on ‘Corrosion properties of duplex stainless steel’, Glasgow, Scotland, November 1994, The Welding Institute (TWI), Paper III.
7. 10.1016/0010-938X(94)00120-U10.1016/0010-938X(94)00120-U ↗
8. 10.1016/S0921-5093(03)00077-710.1016/S0921-5093(03)00077-7 ↗
9. Ord J. L. · J. Electrochem. Soc. · 1976 · 123 · 1976
10. 10.1149/1.208695210.1149/1.2086952 ↗
11. Park H. W. · J. Korean Weld. Join. Soc. · 2002 · 20 · 1
12. Senda T. · Trans. Jpn Weld. Res. Inst. · 1971 · 12 · 45
13. Almar A. ‘Fatigue handbook’, 3rd edn, 259–285; 1985, London, Tapir Academic Press.
14. 10.1016/j.corsci.2009.08.01510.1016/j.corsci.2009.08.015 ↗
15. Lee D. N. ‘Material strength studies’, 2nd edn, 249–251; 1992, Seoul, Munundang.
16. Ha T. H. · J. Corros. Sci. Soc. Korea · 1998 · 27 · 514
17. Kiesheyer H. · Z. Metallkd · 1976 · 67 · 258
18. Jackson E., and Matthews L. M.: Proc. Conf. on ‘The precipitaion kinetics of intermetallic phase in duplex stainless steel and their influence on mechanical properties’, Chiba, Japan, June 1991, The Iron and Steel Institute of Japan (ISIJ), 730.
19. Huhtala T., Nilsson J.O., and Wilson A.: Proc. 4th Int. Conf. on ‘Influence of W and Cu on structural stability in super duplex wled metals’, Glasgow, Scotland, November 1994, The Welding Institute (TWI), Paper 43.
20. Song S. H. · Trans. Korean Soc. Mech. Eng. A · 1997 · 21 · 842