The potential of cast 7075 billets for thixoforging without prior thermomechanical processing was investigated. Slugs machined from EN AW7075 cast billet were thixoformed at 615°C with a liquid fraction of 20. The dendritic as cast matrix has transformed into a more compact structure during heating into the semisolid temperature range. This structural change was facilitated by the reversion of the fine precipitates along the dendrite boundries inherited from dendritic segregation of the as cast billet and the coalescence of the neighbouring dendrite arms. The equiaxed polygonal grains thus obtained have become increasingly globular upon holding at 615°C. The liquid phase penetrated between the grains, forming a more or less continous intergranular network. Microstructural features essential for forming in the semisolid state were obtained after ∼10 min at this temperature. The forming process has taken place in the semisolid state with no evidence of grain deformation. The thixoformed 7075 part was solutionised at 470°C for 6 h and was subsequently quenched in water. Artificial aging at 121°C has produced hardness values as high as 175 HV after 16 h. It is thus fair to conclude that the cast EN AW7075 billet can be readily thixoformed after a 3 min heating ramp and a 10 min isothermal hold at 615°C.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Materials Institute Marmara Research Center, TUBITAK, Gebze, Kocaeli, Turkey
References (25)
Show source-provided references
1. 10.4028/www.scientific.net/MSF.242.1110.4028/www.scientific.net/MSF.242.11 ↗
2. 10.1016/S0921-5093(99)00674-710.1016/S0921-5093(99)00674-7 ↗
3. 10.1016/j.actamat.2003.08.02310.1016/j.actamat.2003.08.023 ↗
4. www.alcoa.com/mill_products/catalog/pdf/alloy7075techsheet.pdf.
5. 10.4028/www.scientific.net/MSF.396-402.39310.4028/www.scientific.net/MSF.396-402.393 ↗
6. 10.1179/1743284711Y.000000004810.1179/1743284711Y.0000000048 ↗
7. 10.1007/BF0266109010.1007/BF02661090 ↗
8. 10.1179/imr.1994.39.5.17310.1179/imr.1994.39.5.173 ↗
9. 10.1179/09506600122500107610.1179/095066001225001076 ↗
10. Kenney MP, Courtois JA, Evans RD, Farrior GM, Kyonka CP, Koch AA, Young KP: ‘Metals handbook’, 9th edn, Vol. 15, 327–338; 1988, Metals Park, OH, ASM International.
11. 10.1016/S0921-5093(00)00908-410.1016/S0921-5093(00)00908-4 ↗
12. 10.1016/0921-5093(95)09861-510.1016/0921-5093(95)09861-5 ↗
13. Garat M, Blais S, Pluchon C, Loue WR:Proc. 5th Int. Conf. on ‘Semi-solid processing of alloys and composites’(, Bhasin A K, et al.), 17; 1998, Golden, CO, School of Mines.
14. 10.1016/S0921-5093(03)00528-810.1016/S0921-5093(03)00528-8 ↗
15. Young KP, Kyonka CP, Courtois JA: ‘Fine grained metal composition’, US Patent 4415374, 1983.
16. 10.1016/j.msea.2004.05.00410.1016/j.msea.2004.05.004 ↗
17. 10.4028/www.scientific.net/MSF.396-402.13110.4028/www.scientific.net/MSF.396-402.131 ↗
18. 10.1016/S0924-0136(02)00818-X10.1016/S0924-0136(02)00818-X ↗
19. 10.1016/j.jmatprotec.2011.05.01610.1016/j.jmatprotec.2011.05.016 ↗
20. 10.3139/146.10143710.3139/146.101437 ↗
21. 10.1016/j.jallcom.2007.07.01610.1016/j.jallcom.2007.07.016 ↗
22. 10.1016/j.jallcom.2007.01.05310.1016/j.jallcom.2007.01.053 ↗
23. 10.4028/www.scientific.net/MSF.519-521.191910.4028/www.scientific.net/MSF.519-521.1919 ↗
24. 10.1016/S0921-5093(03)00056-X10.1016/S0921-5093(03)00056-X ↗
25. 10.1016/S1003-6326(06)60101-510.1016/S1003-6326(06)60101-5 ↗