Effect of fibre surface morphology on stability of C/TiBxcoatings in Ti–6Al–4V/σ (SM1240) fibre metal matrix composite
Source abstract
Abstract
Sigmafibres (SM1240) produced by a chemical vapour deposition process using a 15 μm tungsten wire corefor SiC deposition have a duplex coating of graphitic carbon and TiBx. Nodules present on the fibre surface are attributed to the deposition of the carbon coating over soot particles present on the substrate. Both the carbon and TiBx coatings were stable in vacuum or air at temperatures up to 973 K. The nodules werefound to be sites of preferential attack by the titanium alloy matrix. The average number of nodules per fibre decreased more rapidly when the specimens were heated in air than in vacuum. It is suggested that the nodules may reduce the stability temperature of the coatings.MST/2028
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. SMITH P. R. · J. Met. · 1984 · 36 · 19
2. 10.1177/00219983750090040210.1177/002199837500900402 ↗
3. 10.1016/0956-7151(91)90111-D10.1016/0956-7151(91)90111-D ↗
4. 10.1016/0036-9748(89)90128-210.1016/0036-9748(89)90128-2 ↗
5. MACKAY R. A. · J. Met. · 1991 · 43 · 23
6. 10.1179/imr.1993.38.1.110.1179/imr.1993.38.1.1 ↗
7. 10.1111/j.1365-2818.1993.tb03304.x10.1111/j.1365-2818.1993.tb03304.x ↗
8. 10.1111/j.1365-2818.1993.tb03305.x10.1111/j.1365-2818.1993.tb03305.x ↗
9. 10.1179/mst.1994.10.9.79710.1179/mst.1994.10.9.797 ↗
10. 10.1111/j.1365-2818.1993.tb03306.x10.1111/j.1365-2818.1993.tb03306.x ↗
11. PRAGNELL P. B. · 1992 · 2
12. C. M. WARWICK and J.E. SMITII: in Proc. Conf. 'Processing, microstructure, and properties', (ed. N. Hansen et al.), 735–740; 1991, Roskilde, Denmark, Riso International Laboratory.
13. R. SHATWELL: personal communication, BP Metal Composites, Sunbury Research Centre, Sunbury.
14. 10.1111/j.1151-2916.1964.tb13793.x10.1111/j.1151-2916.1964.tb13793.x ↗
15. F. E. WAWNER: in 'Fibre reinforcement for composite materials', Composite Materials Series, (ed. A. R. Bunsell), Vol. 2, 371–425; 1988, Amsterdam, Elsevier.
16. J. M. BLOCHER: 'Vapor deposition', The Electrochemical Society Series, (ed. C. F. Powell et al.), 650–698; 1966, New York, John Wiley & Sons.
17. J. C. BOKROS: in 'Chemistry and physics of carbon', Vol. 5 (ed. P. L. Walker et al.), 1–118; 1969, New York, Marcel Dekker.
18. 10.1557/JMR.1990.286510.1557/JMR.1990.2865 ↗
19. P. A. TESNER: in 'Chemistry and physics of carbon', Vol. 19, (ed. P. A. Thrower), 65–156; 1984, New York, Marcel Dekker.
20. F. L MARCH and K. Iwo: in 'Introduction to carbon science', (ed. H. Marsh, 107–145; 1989, London, Butterworth.10.1016/B978-0-408-03837-9.50009-9 ↗
21. UPADHYAYA D. · J. Phys. III · 1993 · 3 · 1717
22. UPADHYAYA D. · Mater. Sci. Technol.