Oxide formation during electric resistance welding of low carbon steels
Source abstract
Abstract
The influence of Mn and Cr on the formation of surface oxides and their entrapment during electric resistance welding of Si containing low carbon steels was studied using thermodynamic calculations and experimental investigation of the microstructure of the different oxide inclusions within welds on electric resistance welding-fabricated pipes. The process of oxidation during the welding process, its dependence on oxygen content, temperature of oxidation and the composition of ferrite within the parent steel were analysed. It was shown that the most important influence on the type of oxide inclusions formed during welding is the Mn/Si ratio, while Cr has an indirect influence via carbide formation, which increases the relative content of Mn in ferrite.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Material Properties and Failure Mechanisms · Welding Techniques and Residual Stresses
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Thermochemistry of Materials Scientific Research Centre, NUST MISIS, Leninsky Prosp. 4, 119049 Moscow, Russia
Engineering Technology Centre, AO Vyksa Steel Works, 45 Bratjev Batashevykh St, Vyksa 607060, Russia
Institute for Materials Research, School of Chemical and Process Engineering, University of Leeds, LS2 9JT Leeds, UK
References (18)
Show source-provided references
1. Buckland B. · Piledriver · 2005 · 1 · 20
2. Watanabe S., Ode F., Kano N., Yokoyama E., and Hirano Y. ‘Recent progress in techniques of manufacturing small diameter electric resistance weld tubes’ 4, ‘Kawasaki Steel Technical Report’, 84–96; 1981.
3. 10.1179/mst.1995.11.2.18610.1179/mst.1995.11.2.186 ↗
4. 10.1007/BF0281727710.1007/BF02817277 ↗
5. 10.1016/0921-5093(96)10370-110.1016/0921-5093(96)10370-1 ↗
6. Ramirez J. E. · Res · 2008 · 87 · 65
7. Bhadeshia H. K. D. H., and Svensson L. E. ‘Mathematical modelling of weld phenomena’, (ed. Cerjak H., and Easterling K. E. 109–178; 1993, London, The Institute of Materials.
8. 10.1016/S0364-5916(02)00036-610.1016/S0364-5916(02)00036-6 ↗
9. 10.1007/s11663-997-0029-z10.1007/s11663-997-0029-z ↗
10. 10.1016/j.jallcom.2010.04.25210.1016/j.jallcom.2010.04.252 ↗
11. 10.6028/jres.005.02110.6028/jres.005.021 ↗
12. Eguchi M. · Bull. Res. Inst. Miner. Dressing Metall., Tohoku Univ · 1977 · 33 · 24
13. 10.2355/isijinternational.45.79810.2355/isijinternational.45.798 ↗
14. 10.1111/j.1551-2916.2005.00719.x10.1111/j.1551-2916.2005.00719.x ↗
15. 10.1007/BF0270974910.1007/BF02709749 ↗
16. Verein Deutcher Eisenhuttenleute (VDEh) ‘Slag Atlas’, (ed.), 2nd edn, 1–616; 1995, Verlag Stahleisen GmbH.
17. 10.1007/s11663-000-0134-810.1007/s11663-000-0134-8 ↗
18. 10.1016/S0364-5916(02)00037-810.1016/S0364-5916(02)00037-8 ↗