journal article·1995-10

Sharp boron doping within thin SiGe layer by rapid thermal chemical vapour deposition

B. Tillack, G. Ritter, D. Krüger, P. Zaumseil, G. Morgenstern, K.-D. Glowatzki

Materials Science and Technology· Volume 11· Issue 10
Publisher page

Abstract

Boron δ doping of Si and SiGe has been investigated using rapid thermal chemical vapour deposition from the SiH4–GeH4−H2 system with B2H6 as the B source gas. By incorporation of B into the growing Si film, B peaks with an exponential decay length of 1·7 nm/ decade were prepared. The B peak concentration was found to be dependent on Ge concentration, doping time, and doping temperature. An explanation of the results obtained is proposed based on a transitional behaviour between equilibrium and kinetic control of the process. If the B δ doping is carried out by interrupting the epitaxy, the process is controlled by the surface adsorption equilibrium. Hence B δ layers of about one monolayer thickness were prepared in Si and SiGe with an exponential decay length of 1·4 nm/decade at a temperature of 350°C.MST/3293
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Silicon Nanostructures and Photoluminescence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. 10.1116/1.58683210.1116/1.586832 ↗
2. 10.1116/1.58682710.1116/1.586827 ↗
3. 10.1063/1.10452310.1063/1.104523 ↗
4. 10.1116/1.58682610.1116/1.586826 ↗
5. MUROTA J. · J. Phys. IV · 1993 · 3 · 427
6. 10.1016/0040-6090(93)90148-I10.1016/0040-6090(93)90148-I ↗
7. 10.1016/0022-0248(90)90571-210.1016/0022-0248(90)90571-2 ↗
8. 10.1063/1.35344110.1063/1.353441 ↗
9. 10.1002/sia.74021060210.1002/sia.740210602 ↗
10. KIRCHER R. · J. Phys. IV · 1993 · 1 · 78T
11. 10.1116/1.58628210.1116/1.586282 ↗
12. 10.1063/1.10020610.1063/1.100206 ↗