Grain refinement of AZ91D Mg alloy by a spinning spray of Ar+CO2 mixture gas was investigated. The results have shown that the grain size was refined significantly and effectively by this processing after 15–30 min treatment, but further extension of the treatment did not refine the grain markedly. It was shown that this processing has an ‘aging behaviour’, which means that the refining efficiency declines with the extension of holding time at melting temperature. Although the cooling rate affected the final grain size of AZ91D sample refined by the processing, it did not change the aging behaviour. The effective time is 45–60 min. It was analysed that Al4C3 could act as nucleation site of the primary Mg, which contributes to the grain refinement. Mechanical property testing demonstrated that refinement by the Ar+CO2 processing significantly refined the grain size of the as cast AZ91D samples produced by sand and permanent cast and in turn enhanced the strength and improved the elongation.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and EngineeringJiamusi University, Jiamusi 154007, China;, Email: erlin.zhang@imr.ac.cn

Northeast Light Alloy Co., Ltd, Harbin, 150060, China

School of Materials Science and EngineeringJiamusi University, Jiamusi 154007, China

School of Materials Science and EngineeringHarbin Institute of Technology, Harbin, 150001, China

References (21)

Show source-provided references
1. 10.1179/02670830110150906110.1179/026708301101509061 ↗
2. 10.1016/j.scriptamat.2004.06.02210.1016/j.scriptamat.2004.06.022 ↗
3. 10.1016/j.scriptamat.2006.04.01410.1016/j.scriptamat.2006.04.014 ↗
4. Motegi T. · Magn. Alloys · 2000 · 350 · 191
5. Tamura Y. · Magn. Alloys · 2000 · 350 · 199
6. 10.1016/j.msea.2005.08.21410.1016/j.msea.2005.08.214 ↗
7. 10.1007/BF0283034910.1007/BF02830349 ↗
8. 10.2320/matertrans.44.10710.2320/matertrans.44.107 ↗
9. 10.1016/j.scriptamat.2005.05.00810.1016/j.scriptamat.2005.05.008 ↗
10. 10.1016/j.scriptamat.2003.07.00110.1016/j.scriptamat.2003.07.001 ↗
11. 10.2464/jilm.48.39510.2464/jilm.48.395 ↗
12. 10.1007/s11661-005-0030-610.1007/s11661-005-0030-6 ↗
13. 10.1016/j.scriptamat.2005.09.02210.1016/j.scriptamat.2005.09.022 ↗
14. 10.1016/j.scriptamat.2004.01.01210.1016/j.scriptamat.2004.01.012 ↗
15. 10.1016/j.jallcom.2006.07.11710.1016/j.jallcom.2006.07.117 ↗
16. 10.1016/j.scriptamat.2004.10.03010.1016/j.scriptamat.2004.10.030 ↗
17. 10.1016/j.scriptamat.2004.10.01410.1016/j.scriptamat.2004.10.014 ↗
18. 10.1016/j.scriptamat.2006.02.04810.1016/j.scriptamat.2006.02.048 ↗
19. 10.1016/j.scriptamat.2005.06.01010.1016/j.scriptamat.2005.06.010 ↗
20. Motegi T.: Mater. Sci. Eng. A, 2005, A413-414,408–411.10.1016/j.msea.2005.08.214 ↗
21. 10.2320/matertrans.43.278410.2320/matertrans.43.2784 ↗