journal article·1994-12

Effects of pearlite formation on mechanical properties of austempered ductile iron

M. Bahmani, R. Elliott

Materials Science and Technology· Volume 10· Issue 12
Publisher page

Abstract

Mechanical property measurements are described for a ductile iron alloyed with Mn, Mo, and Cu in the fully austempered condition, andfor irons with various amounts of pearlite introduced by isothermal transformation at 550°C after austenitising at 920°C for 120 min and before austempering at 370°C for 60 min. The ultimate tensile strength, 0·2% proof strength, elongation, impact energy, and hardness all decrease as the amount of pearlite in the structure increases. A smaller amount of pearlite can be tolerated in the alloyed iron compared with an unalloyed iron before itfails to satisfy the standard.MST/2041
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (5)

Show source-provided references
1. MOORE D. J. · AFS Trans. · 1990 · 98 · 449
2. BAYATI H. · Mater. Sci. Technol.
3. 10.1179/mst.1993.9.7.57210.1179/mst.1993.9.7.572 ↗
4. 10.1179/mst.1994.10.1.3510.1179/mst.1994.10.1.35 ↗
5. VIAU R. · AFS Trans. · 1987 · 95 · 171