Stability of ZrO2–Y2O3t′ phase formed during laser sealing

K. Mohammed Jasim, R. D. Rawlings, D. R. F. West

Publisher page

Abstract

Results are reported concerning the effect of thermal treatments in the temperature range 1050–1500°C for 1–1000 h on the stability of the t′ phase present in laser sealed layers of ZrO2–8·5 wt-% Y2O3. Aging for up to 1000 h at 1050°C is not sufficient to cause significant transformation of the t′ phase. At temperatures >1300°C, the t′ phase is less stable and transforms to mixtures of the t and c phases in proportions which are a function of both the time and temperature of aging. An improvement in the fracture toughness of the sealed layer was found to occur when substantial proportions of t phase were produced by annealing.MST/1529
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. 10.1016/0040-6090(80)90513-110.1016/0040-6090(80)90513-1 ↗
2. 10.1179/mst.1985.1.6.41710.1179/mst.1985.1.6.417 ↗
3. 10.1007/BF0103185310.1007/BF01031853 ↗
4. 10.1111/j.1151-2916.1989.tb06103.x10.1111/j.1151-2916.1989.tb06103.x ↗
5. 10.1179/mst.1986.2.3.25710.1179/mst.1986.2.3.257 ↗
6. 10.1007/BF0172933410.1007/BF01729334 ↗
7. 10.1016/0040-6090(85)90219-610.1016/0040-6090(85)90219-6 ↗
8. 10.1007/BF0055529610.1007/BF00555296 ↗
9. 10.1179/mst.1989.5.9.86510.1179/mst.1989.5.9.865 ↗
10. 10.1179/mst.1989.5.10.96110.1179/mst.1989.5.10.961 ↗
11. R. STEVENS: ‘An introduction to zirconia’, 2 edn, 1; 1986, Manchester, Magnesium Elektron.
12. 10.1149/1.277821910.1149/1.2778219 ↗
13. SRIVASTAVA K. K. · Trans. J. Br. Ceram. Soc., · 1974 · 73 · 85
14. 10.1111/j.1151-2916.1978.tb09220.x10.1111/j.1151-2916.1978.tb09220.x ↗
15. 10.1111/j.1151-2916.1983.tb09961.x10.1111/j.1151-2916.1983.tb09961.x ↗
16. 10.1246/bcsj.43.261410.1246/bcsj.43.2614 ↗
17. SKAGGS S. R. · Bull. Am. Ceram. Soc., · 1972 · 51 · 324