journal article·1986-11

Joining Si3N4to type 405 steel with soft metal interlayers

K. Suganuma, T. Okamoto, Y. Miyamoto, M. Shimada, M. Koizumi

Materials Science and Technology· Volume 2· Issue 11
Publisher page

Abstract

The suitability of four pure metals, Ni, Fe, Ti, and Nb, as interlayers for bonding silicon nitride to type 405 ferritic stainless steel has been examined. Bonding was carried out by hot isostatic pressing at temperatures between 1473 and 1673 K under a pressure of 100 MPa. Of the metals tested, Fe and Nb formed the strongest interfacial bonds with Si3N4. To reduce the influence of residual stress in joints, Fe/W and Nb/W laminated interlayers were also examined. The use of W restricted the contraction of Fe or Nb, and the Si3N4/steel joints with these interlayers had a tensile strength of more than 50 MN m−2. A low-pressure (10 MPa) bonding process was also used for the Fe/W interlayer.MST/470
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. 10.1007/BF0055244410.1007/BF00552444 ↗
2. SUGANUMA K. · High Temp. High Press., · 1985 · 16 · 627
3. 10.1111/j.1151-2916.1984.tb19688.x10.1111/j.1151-2916.1984.tb19688.x ↗
4. 10.1016/0022-3115(85)90255-710.1016/0022-3115(85)90255-7 ↗
5. HATAKEYAMA F. · J. Mater. Sci., 1986, to be published.
6. 10.1007/BF0072005710.1007/BF00720057 ↗
7. KLOMP Y. · Weld. J., · 1971 · 50 · 88s
8. 10.1007/BF0120350510.1007/BF01203505 ↗
9. SUGANUMA K. · High Temp. Sci., · 1985 · 20 · 127
10. L. F. VOITOVICH: ‘Refractory compounds’, 96-103; 1971, Kiev, Naukovy Dumka.
11. SUGANUMA K. · Adv. Ceram. Mater. · 1986
12. 10.1007/BF0072041610.1007/BF00720416 ↗