journal article·2026-04

Comparison of the effects of low temperature austempering (LTA), quenching & partitioning (Q&P) and quenching & tempering (Q&T) processes on wear performance in high silicon cast steel

Burak Nalcaci, Tolga Yilmaz, Onur Okur, Ahmet Gural, Mehmet Erdogan

Materials Science and Technology· Volume 42· Issue 5
Publisher page

Abstract

The present study was undertaken to investigate the wear performance of Low Temperature Austempering (LTA), Quenching and Partitioning (Q&P) and Quenching and Tempering (Q&T) processes in high silicon cast steel. With this object, the high silicon cast steel samples were produced by casting sand mold in a Y block shape and subsequently normalized at 910 °C. Within the scope of heat treatment studies, the samples were austenitized at 900 °C for 30 min, and the first batch of samples was austempered in a salt bath at 280 °C for 120 min for low temperature austempering process. After austenitizing at the same conditions, the second batch of samples was exposed to oil quenching at 180 °C for 10 min followed by partitioning at 280 °C in a salt bath for 110 min to keep applied heat treatment time the same. As Quenching and Tempering process is frequently used when the wear properties comes, as a benchmark group third batch samples were quenched in oil at room temperature for a few minutes and tempered at 280 °C for 120 min. In the characterization studies, ball on disc tribometer, hardness test, XRD analysis, optical microscope, Field Emission-Scanning Electron Microscope (FE-SEM) and optical profilometer were utilized. The findings of this study indicated that while austempered samples consisted of carbide free bainitic structure (CFB), the samples went through a Q&P process included tempered martensite as well as CFB structure. The third group samples quenched and tempered contained tempered martensite. The lowest amount of austenite was determined in the Q&T process with about 11%, while approximately 17% volume austenite was determined in both Q&P and LTA processes. In general, both LTA and Q&P processes considerably increased the wear performance compared to the normalized condition and Q&P process is superior to LTA process and is a very competitive option in terms of wear resistance against Q&T process.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Gazi University

Kirikkale University

References (36)

Show source-provided references
1. 10.1016/j.rinma.2023.10043010.1016/j.rinma.2023.100430 ↗
2. 10.1016/j.jmrt.2023.05.06710.1016/j.jmrt.2023.05.067 ↗
3. 10.1016/j.jmrt.2020.03.00310.1016/j.jmrt.2020.03.003 ↗
4. 10.1016/j.wear.2016.12.03810.1016/j.wear.2016.12.038 ↗
5. 10.1179/174328408X27597310.1179/174328408X275973 ↗
6. 10.1016/j.msea.2012.08.08310.1016/j.msea.2012.08.083 ↗
7. 10.1016/j.actamat.2023.11874210.1016/j.actamat.2023.118742 ↗
8. 10.1016/j.jmrt.2022.04.06610.1016/j.jmrt.2022.04.066 ↗
9. 10.1016/j.triboint.2022.10807110.1016/j.triboint.2022.108071 ↗
10. 10.1016/j.matpr.2017.08.02410.1016/j.matpr.2017.08.024 ↗
11. 10.1007/s12633-020-00513-210.1007/s12633-020-00513-2 ↗
12. 10.1016/j.msea.2022.14455310.1016/j.msea.2022.144553 ↗
13. 10.1016/j.msea.2009.02.01310.1016/j.msea.2009.02.013 ↗
14. 10.1016/j.msea.2023.14518610.1016/j.msea.2023.145186 ↗
15. 10.1007/s12666-022-02818-910.1007/s12666-022-02818-9 ↗
16. 10.1016/j.wear.2018.12.00610.1016/j.wear.2018.12.006 ↗
17. 10.1016/j.wear.2020.20333610.1016/j.wear.2020.203336 ↗
18. 10.55713/jmmm.v30i4.92510.55713/jmmm.v30i4.925 ↗
19. 10.1080/03019233.2019.166652610.1080/03019233.2019.1666526 ↗
20. 10.3390/ma1424751810.3390/ma14247518 ↗
21. 10.1016/j.wear.2017.12.01610.1016/j.wear.2017.12.016 ↗
22. 10.1016/j.msea.2022.14321210.1016/j.msea.2022.143212 ↗
23. 10.1016/j.msea.2016.08.02610.1016/j.msea.2016.08.026 ↗
24. 10.1080/03019233.2023.220426810.1080/03019233.2023.2204268 ↗
25. 10.1016/j.mtcomm.2022.10503110.1016/j.mtcomm.2022.105031 ↗
26. 10.1016/j.wear.2020.20335910.1016/j.wear.2020.203359 ↗
27. 10.1016/j.wear.2022.20451210.1016/j.wear.2022.204512 ↗
28. Astm A. E975, Standard Practice for X-Ray Determination of Retained Austenite in Steel with Near Random Crystallographic Orientation 1. Astm 2013; 03: –7.
29. 10.1007/s11665-020-04699-910.1007/s11665-020-04699-9 ↗
30. 10.1134/S0031918X2360002110.1134/S0031918X23600021 ↗
31. 10.1515/secm-2020-004510.1515/secm-2020-0045 ↗
32. 10.1016/j.wear.2016.04.01210.1016/j.wear.2016.04.012 ↗
33. 10.1016/j.msea.2016.03.00610.1016/j.msea.2016.03.006 ↗
34. 10.1016/j.msea.2012.03.09810.1016/j.msea.2012.03.098 ↗
35. 10.1080/03019233.2021.199065010.1080/03019233.2021.1990650 ↗
36. 10.1016/j.matdes.2014.02.03510.1016/j.matdes.2014.02.035 ↗