journal article·2021-03

Microstructure and mechanical properties of pure Mg after spiral equal-channel extrusion

Jinghui Li, Fuguo Li, Shan Liang, Zhenyi Huang, Mingya Zhang

Materials Science and Technology· Volume 37· Issue 4
Publisher page

Abstract

One of the severe plastic deformation techniques, elliptical cross-sectioned spiral equal-channel extrusion (ECSEE) was successfully applied to the pure Mg processed at 200°C and the microstructure and properties were studied. The observation shows that the grains are refined to 2.1 µm after 2-pass deformation. The proportion of high-angle grain boundary increases to 49.4% after 6-pass. The minimum time of grain boundary rotating 30° is about 0.847 ms, and the maximum time is 2.34 ms. TEM observation illustrates the grain morphology evolves from shear bands to recrystallised grains. There was a significant increase in strength to ∼180 MPa but a decrease in the ductility (∼12%) of pure Mg after 6-pass ECSEE. The refinement mechanism is mainly divided into mechanical and physical refinement.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Metallurgical Engineering, Anhui University of Technology, Ma'anshan, People's Republic of China

State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an, People's Republic of China

School of Innovative Education, Anhui University of Technology, Ma'anshan, People's Republic of China

Funding

National Natural Science Foundation of China · Research Fund of Key Laboratory of Advanced Metal Material Green Preparation and Surface Technology (AHUT), Ministry of Education, China · Postdoctoral Fund from Jiangsu Province and Anhui Province

References (35)

Show source-provided references
1. 10.1016/j.actamat.2016.09.05410.1016/j.actamat.2016.09.054 ↗
2. 10.1016/j.msea.2017.06.07610.1016/j.msea.2017.06.076 ↗
3. 10.1016/j.jmatprotec.2017.03.02510.1016/j.jmatprotec.2017.03.025 ↗
4. 10.1016/j.matpr.2019.10.08810.1016/j.matpr.2019.10.088 ↗
5. 10.1016/j.actamat.2019.01.02710.1016/j.actamat.2019.01.027 ↗
6. 10.1016/j.mechmat.2020.10332110.1016/j.mechmat.2020.103321 ↗
7. 10.1016/S1674-4799(09)60096-010.1016/S1674-4799(09)60096-0 ↗
8. 10.1016/j.msea.2019.03.10610.1016/j.msea.2019.03.106 ↗
9. 10.1016/j.msea.2009.07.06310.1016/j.msea.2009.07.063 ↗
10. 10.1016/j.jma.2019.11.00410.1016/j.jma.2019.11.004 ↗
11. Torbatisarraf H · Corros Sci · 2019 · 154
12. Castro MM · J Alloys Compd · 2019 · 804
13. Plumeri JE · Procedia Eng · 2017 · 207
14. Wang C · Mater Sci Eng A · 2012 · 548
15. Wang C · Mater Des · 2013 · 43
16. 10.1007/s11665-015-1731-710.1007/s11665-015-1731-7 ↗
17. 10.4172/0976-4860.100020510.4172/0976-4860.1000205 ↗
18. 10.1016/S1875-5372(13)60055-710.1016/S1875-5372(13)60055-7 ↗
19. 10.1016/j.cja.2012.12.01210.1016/j.cja.2012.12.012 ↗
20. 10.1016/j.msea.2014.04.10310.1016/j.msea.2014.04.103 ↗
21. 10.1016/j.msea.2020.13900210.1016/j.msea.2020.139002 ↗
22. 10.1016/j.msec.2019.11054310.1016/j.msec.2019.110543 ↗
23. 10.1016/j.jallcom.2018.01.41210.1016/j.jallcom.2018.01.412 ↗
24. 10.1016/j.jma.2017.05.00210.1016/j.jma.2017.05.002 ↗
25. Zhang W · Acta Mater · 2017 · 134
26. 10.1016/j.msea.2019.13887110.1016/j.msea.2019.138871 ↗
27. 10.1016/j.msea.2008.03.05710.1016/j.msea.2008.03.057 ↗
28. 10.1016/j.msea.2014.04.08310.1016/j.msea.2014.04.083 ↗
29. 10.1016/j.actamat.2019.09.01110.1016/j.actamat.2019.09.011 ↗
30. 10.1016/S0921-5093(01)01160-110.1016/S0921-5093(01)01160-1 ↗
31. 10.1016/S0921-5093(00)01660-910.1016/S0921-5093(00)01660-9 ↗
32. 10.1016/j.matpr.2019.10.08810.1016/j.matpr.2019.10.088 ↗
33. 10.1166/nnl.2009.104410.1166/nnl.2009.1044 ↗
34. 10.1557/JMR.1992.213110.1557/JMR.1992.2131 ↗
35. 10.1016/0036-9748(78)90313-710.1016/0036-9748(78)90313-7 ↗