Sintering behaviour of Nb–16Si–25Ti–8Hf–2Cr–2Al alloy powder fabricated by a hydrogenation–dehydrogenation method

Ki Beom Park, Jaeho Choi, Sung Yong Lee, Jae-Young Park, Tae-Wook Na, Jong-In Choi, Jang-Won Kang, Hyung-Ki Park

Materials Science and Technology· Volume 36· Issue 12
Publisher page

Abstract

The present study investigated the sintering behaviour of Nb–16Si–25Ti–8Hf–2Cr–2Al alloy powders. The alloy powders were produced using ahydrogenation–dehydrogenation method and featured an irregular morphology. Powders sintered at 1500°C and 1600°C exhibited pores in their microstructures, while powders sintered at 1700°C for 4 h were fully densified and poreless. The cast ingot and powders were composed of three phases: Nb ss , Nb 5 Si 3 , and Nb 3 Si. However, the Nb 3 Si phase was not observed, while HfO 2 oxides formed in the sintered compact. The hafnium and oxygen reacted to form an HfO 2 oxide during the high-temperature sintering process. From the result of the thermodynamic calculation, Hf oxide formed after sintering because Hf has the highest driving force for oxidation among the elements constituting the alloy.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · MXene and MAX Phase Materials · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Functional Materials and Components R&D Group, Gangwon Division, Korea Institute of Industrial Technology, Gangneung, Republic of Korea

Department of Advanced Metal and Materials Engineering, Gangneung-Wonju National University, Gangneung, Republic of Korea

Funding

Creative Materials Discovery Program · National Research Foundation of Korea · Ministry of Science · Gangneung-Wonju National University

References (24)

Show source-provided references
1. 10.1007/s11661-003-0269-810.1007/s11661-003-0269-8 ↗
2. 10.1016/0257-8972(89)90099-610.1016/0257-8972(89)90099-6 ↗
3. 10.1016/j.combustflame.2006.01.00910.1016/j.combustflame.2006.01.009 ↗
4. 10.1007/BF0322136110.1007/BF03221361 ↗
5. 10.1016/j.msea.2007.08.03510.1016/j.msea.2007.08.035 ↗
6. 10.1007/BF0259562910.1007/BF02595629 ↗
7. 10.1557/PROC-322-49110.1557/PROC-322-491 ↗
8. 10.1007/BF0266737010.1007/BF02667370 ↗
9. 10.1007/s11661-003-0149-210.1007/s11661-003-0149-2 ↗
10. 10.1557/PROC-364-133910.1557/PROC-364-1339 ↗
11. 10.1016/j.msea.2006.09.13510.1016/j.msea.2006.09.135 ↗
12. 10.1007/s11661-004-0370-710.1007/s11661-004-0370-7 ↗
13. 10.1016/j.corsci.2013.01.01010.1016/j.corsci.2013.01.010 ↗
14. 10.1007/BF0322136010.1007/BF03221360 ↗
15. 10.1007/s11837-999-0077-810.1007/s11837-999-0077-8 ↗
16. 10.1016/S0921-5093(02)00011-410.1016/S0921-5093(02)00011-4 ↗
17. 10.1016/j.corsci.2019.10828110.1016/j.corsci.2019.108281 ↗
18. Chen Z, Yan YW. Influence of sintering temperature on microstructures of Nb/Nb5Si3 in situ composites synthesized by spark plasma sintering. JALCOM. 2006; 413:73–76.
19. 10.1016/j.pnsc.2013.01.00910.1016/j.pnsc.2013.01.009 ↗
20. 10.3390/met912129610.3390/met9121296 ↗
21. 10.1016/j.jallcom.2019.15275710.1016/j.jallcom.2019.152757 ↗
22. 10.3390/met911115410.3390/met9111154 ↗
23. 10.1016/j.matlet.2019.03.13410.1016/j.matlet.2019.03.134 ↗
24. 10.3390/ma1221354910.3390/ma12213549 ↗