journal article·2004-10

Analysis of high flow stress and microstructural evolution of TC6 titanium alloy during isothermal forging

A.-M. Xiong, M.-Q. Li, W.-C. Huang, S.-H. Chen, H. Lin

Materials Science and Technology· Volume 20· Issue 10
Publisher page

Abstract

Elevated temperature true stress – strain curves have been determined for the isothermal deformation of a TC6 titanium alloy using hot compression testing in the deformation temperature range 800 – 1040°C, strain rate range 0.001 – 50 s-1 and reduction in height of 30 – 50%. The experimental results show that the flow stress of TC6 titanium alloy is strongly dependent on process parameters, especially on the deformation temperature and strain rate. The peak stress and steady stress of such an alloy have the same characterisation, which increases with higher strain rate and lower deformation temperature. During isothermal forging, microstructural characterisation, including volume fraction, grain size, and grain pattern of prior α phase, varies with different temperatures, height reductions, and strain rates.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgy and Material Forming · Titanium Alloys Microstructure and Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (5)

Show source-provided references
1. 10.1179/mst.1997.13.3.20310.1179/mst.1997.13.3.203 ↗
2. 10.1179/mst.1997.13.3.21010.1179/mst.1997.13.3.210 ↗
3. 10.1016/S0921-5093(00)00741-310.1016/S0921-5093(00)00741-3 ↗
4. 10.1115/1.290413110.1115/1.2904131 ↗
5. 10.1179/mst.1998.14.4.33910.1179/mst.1998.14.4.339 ↗