journal article·1999-01

Improvement of formability of leaded α brass during hot working

T. Yano, X. Ling, K. Higashida, K. Higashida, R. Onodera

Materials Science and Technology· Volume 15· Issue 1
Publisher page

Abstract

Isothermal hot compression tests with a strain rate of 0·1–0·4 s-1 were carried out at 973 K on an α brass alloy containing 0–1·5 wt-% lead. The fracture behaviour was strongly dependent on both lead content and grain size. In leaded α brass, fracture occurred easily when the grain size was larger than ∼100 μm. In non-leaded α brass, no fracture was observed at any grain size. In the leaded brass, fracture occurred only at the free surface and was attributed to grain boundary sliding. The poor formability of leaded α brass was markedly improved by changing the phase of the specimen surface from α to β brass. This result suggests that the surface β phase suppressed the grain boundary sliding of the α grains.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgy and Material Science · Metallurgy and Material Forming · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (9)

Show source-provided references
1. KOCH C. C. · Trans. ASM · 1964 · 57 · 519—526
2. 10.2320/materia1962.18.1510.2320/materia1962.18.15 ↗
3. 10.1007/BF0055714210.1007/BF00557142 ↗
4. MUTO A. · J. Jpn Inst. Met · 1994 · 58 · 14610.2320/jinstmet1952.58.2_146 ↗
5. MUTO A. · J. Jpn Inst. Met · 1995 · 59 · 2310.2320/jinstmet1952.59.1_23 ↗
6. BAUER O. · Z. Metaad · 1929 · 21 · 145
7. PEROVIC D. D. · Metall · 1987 · 21 · 34510.1016/0036-9748(87)90226-2 ↗
8. 10.1016/0956-716X(93)90108-510.1016/0956-716X(93)90108-5 ↗
9. 10.1007/BF0054980410.1007/BF00549804 ↗