Using heat treatment effects and EBSD analysis to tailor microstructure of hybrid Mg nanocomposite for enhanced overall mechanical response
Source abstract
Abstract
In this study, a detailed investigation on the effect of heat treatment on the microstructural characteristics, texture evolution and mechanical properties of Mg–(5·6Ti+2·5B4C)BM hybrid nanocomposite is presented. Optimised heat treatment parameters, namely, heat treatment temperature and heat treatment time, were first identified through grain size and microhardness measurements. Initially, heat treatment of composites was conducted at temperature range between 100 and 300°C for 1 h. Based on optical microscopic analysis and microhardness measurements, it was evident that significant grain growth and reduction in microhardness occurred for temperatures >200°C. The cutoff temperature that caused significant grain growth/matrix softening was thus identified. Second, at constant temperature (200°C), the effect of variation of heat treatment time was carried out (ranging between 1 and 5 h) so as to identify the range wherein increase in average grain size and reduction in microhardness occurred. Furthering the study, the effect of optimised heat treatment parameters (200°C, 5 h) on the microstructural texture evolution and hence, on the tensile and compressive properties of the Mg–(5·6Ti+2·5B4C)BM hybrid nanocomposite was carried out. From electron backscattered diffraction (EBSD) analysis, it was identified that the optimised heat treatment resulted in recrystallisation and residual stress relaxation, as evident from the presence of ∼87 strain free grains, when compared to that observed in the non-heat treated/as extruded condition (i.e. 2·2 times greater than in the as extruded condition). For the heat treated composite, under both tensile and compressive loads, a significant improvement in fracture strain values (∼60 increase) was observed when compared to that of the non-heat treated counterpart, with ∼20 reduction in yield strength. Based on structure–property correlation, the change in mechanical characteristics is identified to be due to: (1) the presence of less stressed matrix/reinforcement interface due to the relief of residual stresses and (2) texture weakening due to matrix recrystallisation effects, both arising due to heat treatment.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Mechanical Engineering, National University of Singapore (NUS), 9 Engineering Drive 1, Singapore 117 576, Singapore
Department of Materials Engineering, Indian Institute of Science (IISc), Bangalore – 560012, India
Materials Science & Engineering, University of Leeds, Leeds, UK
References (41)
Show source-provided references
1. 10.1002/978047090509810.1002/9780470905098 ↗
2. 10.1023/B:JMSC.0000043583.47148.3110.1023/B:JMSC.0000043583.47148.31 ↗
3. 10.1007/s10853-010-5010-610.1007/s10853-010-5010-6 ↗
4. 10.1002/352760811710.1002/3527608117 ↗
5. 10.1179/imr.1994.39.1.110.1179/imr.1994.39.1.1 ↗
6. 10.1016/0010-4361(94)90222-410.1016/0010-4361(94)90222-4 ↗
7. 10.1016/S1359-835X(02)00049-010.1016/S1359-835X(02)00049-0 ↗
8. 10.1016/S0263-8223(00)00031-310.1016/S0263-8223(00)00031-3 ↗
9. 10.1016/S1359-6462(02)00551-110.1016/S1359-6462(02)00551-1 ↗
10. 10.1179/1743284711Y.000000010810.1179/1743284711Y.0000000108 ↗
11. 10.1179/174328407X23691310.1179/174328407X236913 ↗
12. 10.1016/j.compscitech.2007.10.05710.1016/j.compscitech.2007.10.057 ↗
13. 10.1016/j.jallcom.2005.10.00510.1016/j.jallcom.2005.10.005 ↗
14. 10.1007/s10853-005-0886-210.1007/s10853-005-0886-2 ↗
15. 10.1016/j.msea.2007.02.12210.1016/j.msea.2007.02.122 ↗
16. 10.1016/j.actamat.2010.07.02810.1016/j.actamat.2010.07.028 ↗
17. 10.1016/j.jallcom.2011.04.08310.1016/j.jallcom.2011.04.083 ↗
18. 10.1016/j.matchar.2012.10.00510.1016/j.matchar.2012.10.005 ↗
19. 10.1016/j.jallcom.2013.04.09510.1016/j.jallcom.2013.04.095 ↗
20. 10.1016/j.matchemphys.2013.11.01910.1016/j.matchemphys.2013.11.019 ↗
21. ASM: ‘Binary alloy phase diagram’, 2nd edn., Plus Updates; 1996, Materials Park, OH, ASM International.
22. 10.1023/A:100660270321610.1023/A:1006602703216 ↗
23. 10.1016/S0167-577X(02)00568-210.1016/S0167-577X(02)00568-2 ↗
24. Humphreys FJ and Hatherly M: ‘Recrystallization and related annealing phenomena’; 1995, Oxford, Elsevier.10.1016/B978-0-08-041884-1.50017-9 ↗
25. 10.1179/02670830322500215410.1179/026708303225002154 ↗
26. 10.1016/j.compstruct.2004.11.01010.1016/j.compstruct.2004.11.010 ↗
27. 10.1016/S0079-6425(99)00010-910.1016/S0079-6425(99)00010-9 ↗
28. 10.1179/02670839910150518510.1179/026708399101505185 ↗
29. ‘Standard test method for microindentation hardness of materials’, ASTM E384-11e1, ASTM International, West Conshohocken, PA, USA, 2011.
30. ‘Standard test methods for tension testing of metallic materials’, ASTM E8/E8M-13a, ASTM International, West Conshohocken, PA, USA, 2013.
31. ‘Standard test methods of compression testing of metallic materials at room temperature’, ASTM E9-09, ASTM International, West Conshohocken, PA, USA, 2009.
32. Callister WD and Rethwisch DG: ‘Materials science and engineering: an introduction’; 2007, New York, John Wiley & Sons.
33. Dieter GE: ‘Mechanical metallurgy’; 1976, New York, McGraw-Hill.
34. Chawla KK and Chawla N: ‘Metal–matrix composites’; 2004, New York, Wiley Online Library.10.1002/0471238961.1305200103080123.a01.pub2 ↗
35. 10.1007/BF0108650510.1007/BF01086505 ↗
36. 10.1016/j.msea.2012.03.09910.1016/j.msea.2012.03.099 ↗
37. 10.1016/j.msea.2010.07.08110.1016/j.msea.2010.07.081 ↗
38. 10.4028/www.scientific.net/MSF.467-470.35710.4028/www.scientific.net/MSF.467-470.357 ↗
39. 10.1016/j.actamat.2010.01.05110.1016/j.actamat.2010.01.051 ↗
40. 10.1016/j.msea.2005.01.00210.1016/j.msea.2005.01.002 ↗
41. 10.1016/j.msea.2009.07.00810.1016/j.msea.2009.07.008 ↗