Abstract

This paper presents a novel method for the first stage gas turbine blades lifetime extension based on degraded GTD-111 substrates hardness evolution after the rejuvenation heat treatments (RHTs) process. Moreover, the RHT impact on directionally solidified (DS) GTD-111 nickel-based suparalloys homogenisation and blades hardness properties were revealed and discussed. The measured hardness values indicate that turbine blades hardness progress is closely related to the nucleation of topologically close packed (TCP) phases, irregular γ’ (Ni 3 , Al) precipitates growth, and Cr-rich M 23 C 6 Coarsening at grain boundaries. Aspects like γ′/γ eutectic regions rafting, cooling holes oxidation attacks, and formation of cavities within γ-matrix were also identified and analysed.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Laboratory of Petroleum Equipment's Reliability and Materials, Hydrocarbons and Chemistry Faculty, Université M'Hamed Bougara de Boumerdès, UMBB, Boumerdès, Algeria

References (20)

Show source-provided references
1. 10.1243/095765000153829010.1243/0957650001538290 ↗
2. Lipiak G, Bussmann S, Steinwachs C Lifetime extension for Siemens gas turbines. In: Power Gen Europe, 2006.
3. 10.2514/1.B3437510.2514/1.B34375 ↗
4. Cheruvu NS · ASME Inter Gas Turb Aero Cong Exh · 1999 · 4 · V004T01A008
5. 10.7449/2004/Superalloys_2004_163_17110.7449/2004/Superalloys_2004_163_171 ↗
6. 10.1016/j.msea.2007.06.01010.1016/j.msea.2007.06.010 ↗
7. 10.1016/j.msea.2017.01.00510.1016/j.msea.2017.01.005 ↗
8. 10.1016/j.msea.2009.09.01610.1016/j.msea.2009.09.016 ↗
9. Shuaeib FM, Benyounis KY, Hashmi MSJ. Material behavior and performance in Environments of extreme pressure and temperatures, 2017.10.1016/B978-0-12-803581-8.04170-9 ↗
10. 10.1016/j.matdes.2012.09.01110.1016/j.matdes.2012.09.011 ↗
11. 10.1080/09603409.2017.137791010.1080/09603409.2017.1377910 ↗
12. 10.1080/02670836.2017.141961210.1080/02670836.2017.1419612 ↗
13. 10.3139/146.11085610.3139/146.110856 ↗
14. Wood MI. · Life Assess Hot Sect Gas Turbine Compon · 1999 · 731 · 237
15. 10.1007/s12206-012-0506-410.1007/s12206-012-0506-4 ↗
16. 10.1115/GT2011-4676610.1115/GT2011-46766 ↗
17. Zhang P · J Alloys Comp · 2016 · 09 · 303
18. Lu B. · 2014
19. 10.1016/j.msea.2015.02.05610.1016/j.msea.2015.02.056 ↗
20. 10.1016/S1003-6326(11)60995-310.1016/S1003-6326(11)60995-3 ↗