Characteristics evaluation of SiC/Si nanocomposites produced by spark plasma sintering
Source abstract
Abstract
SiC–Si composites are widely used either as a bulk material or as a matrix for fibre reinforced ceramics. In the current research, nanocomposites of SiC–Si with different volume fractions of Si were sintered by spark plasma sintering (SPS) for the first time. The effect of Si content and different sintering parameters on relative density, microstructure, hardness and fracture toughness of the sintered materials have been investigated. The relative density increased from about 83 to 99% by increasing the sintering temperature to 1700°C, sintering time to 10 min, and pressure to 70 MPa for composites containing >20 vol.-% Si. The results revealed that the full dense SiC–20 vol.-%Si composite can be obtained by SPS at 1700°C, 10 min and 70 MPa. Moreover, in this condition, the hardness and toughness of the composites reached the optimum values.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Materials Science and Engineering, Engineering Faculty, Ferdowsi University of Mashhad, Mashhad, Iran
Universität Stuttgart, Institut für Fertigungstechnologie keramischer Bauteile (IFKB) Stuttgart, Germany
Department of Inorganic Chemistry, Arrhenius Laboratory, Stockholm University Stockholm, Sweden
References (31)
Show source-provided references
1. 10.1111/j.1151-2916.1990.tb06493.x10.1111/j.1151-2916.1990.tb06493.x ↗
2. 10.1021/nl049928610.1021/nl0499286 ↗
3. 10.1016/j.ceramint.2011.01.03310.1016/j.ceramint.2011.01.033 ↗
4. 10.1111/j.1151-2916.1956.tb15609.x10.1111/j.1151-2916.1956.tb15609.x ↗
5. Popper P. The preparation of dense self-bonded silicon carbide, Special ceramic, 1960. https://www.tandfonline.com/doi/pdf/10.1179/pom.1961.4.8.009.
6. 10.1002/(SICI)1521-4052(199908)30:8<480::AID-MAWE480>3.0.CO;2-X10.1002/(SICI)1521-4052(199908)30:8<480::AID-MAWE480>3.0.CO;2-X ↗
7. Lynen A, Larsen J, Clemens M. Verfahren zum herstellen von formkörpern aus reaktionsgebundenem, mit silicium infiltriertem siliciumcarbid und/oder borcarbid und so hergestellter formkörper, Patent WO2015055264A2, 2013. https://patents.google.com/patent/WO2015055264A2.
8. 10.1016/j.procir.2016.02.26910.1016/j.procir.2016.02.269 ↗
9. 10.1016/j.mser.2008.09.00310.1016/j.mser.2008.09.003 ↗
10. 10.1016/j.matdes.2017.01.06410.1016/j.matdes.2017.01.064 ↗
11. 10.1016/j.ceramint.2012.01.01110.1016/j.ceramint.2012.01.011 ↗
12. 10.1016/j.ceramint.2013.02.02910.1016/j.ceramint.2013.02.029 ↗
13. 10.1007/s10853-014-8095-510.1007/s10853-014-8095-5 ↗
14. 10.1111/j.1151-2916.1981.tb10320.x10.1111/j.1151-2916.1981.tb10320.x ↗
15. Harper CA. · 2001
16. 10.1109/JMEMS.2009.203969710.1109/JMEMS.2009.2039697 ↗
17. 10.1002/1521-4079(200211)37:11<1234::AID-CRAT1234>3.0.CO;2-X10.1002/1521-4079(200211)37:11<1234::AID-CRAT1234>3.0.CO;2-X ↗
18. 10.1016/j.jallcom.2015.05.05910.1016/j.jallcom.2015.05.059 ↗
19. 10.1016/j.ijrmhm.2008.02.00310.1016/j.ijrmhm.2008.02.003 ↗
20. 10.1016/j.ceramint.2016.02.05010.1016/j.ceramint.2016.02.050 ↗
21. 10.1016/j.jeurceramsoc.2016.04.02910.1016/j.jeurceramsoc.2016.04.029 ↗
22. 10.1016/j.msea.2012.05.02010.1016/j.msea.2012.05.020 ↗
23. 10.1016/j.ceramint.2018.02.03310.1016/j.ceramint.2018.02.033 ↗
24. 10.1111/j.1151-2916.1995.tb08246.x10.1111/j.1151-2916.1995.tb08246.x ↗
25. 10.1016/j.scriptamat.2017.02.03110.1016/j.scriptamat.2017.02.031 ↗
26. 10.1016/j.ceramint.2016.11.20410.1016/j.ceramint.2016.11.204 ↗
27. 10.1016/j.jeurceramsoc.2017.09.02910.1016/j.jeurceramsoc.2017.09.029 ↗
28. 10.1016/S1003-6326(07)60226-X10.1016/S1003-6326(07)60226-X ↗
29. 10.1016/j.msea.2014.10.06210.1016/j.msea.2014.10.062 ↗
30. 10.1016/j.ijrmhm.2018.07.00810.1016/j.ijrmhm.2018.07.008 ↗
31. 10.1016/j.ijrmhm.2018.03.00610.1016/j.ijrmhm.2018.03.006 ↗