Differences in service-exposed and artificially aged microstructure and tensile properties of ASTM A204 Grade C steel
Source abstract
Abstract
Microstructural characterisation of artificially aged and service-exposed ASTM A204 Grade C steel reveals changes in the cementite particles of pearlite and microstructure. The ageing temperatures were chosen to be high enough to replicate the service degradation but below A c1 to avoid austenitisation in the inter-critical regime. Tensile testing of artificially aged materials shows a decrease in the ultimate tensile strength (UTS) along with an increase in elongation. On the other hand, service-exposed material resulted in an increase in UTS and a decrease in elongation. The softening of pearlite due to spheroidisation of cementite and segregation of alloying elements towards grain boundaries were responsible for the lower UTS of the artificially aged samples. Whereas, the increase in UTS in the service-exposed sample was attributed to the formation of nano-sized carbides inside ferrite grains, hence strengthening the steel matrix.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Chemical and Materials Engineering, University of Alberta, Edmonton, Canada
Suncor Energy, Calgary, Canada
Funding
Suncor Energy Incorporated
References (24)
Show source-provided references
1. Shibli A. · 2014
2. 10.2355/isijinternational.41.62610.2355/isijinternational.41.626 ↗
3. 10.1007/b8064110.1007/b80641 ↗
4. 10.1016/S1044-5803(01)00147-410.1016/S1044-5803(01)00147-4 ↗
5. 10.1016/j.msea.2014.11.02010.1016/j.msea.2014.11.020 ↗
6. 10.1016/j.ijhydene.2017.07.23710.1016/j.ijhydene.2017.07.237 ↗
7. 10.1016/j.ijhydene.2015.07.09510.1016/j.ijhydene.2015.07.095 ↗
8. 10.1115/PVP2013-9709510.1115/PVP2013-97095 ↗
9. 10.1115/1.402995810.1115/1.4029958 ↗
10. 10.1115/1.400456410.1115/1.4004564 ↗
11. Chen J. Fatigue behaviour of coke drum materials and its application to extend the service lives of coke drums [PhD dissertation]. University of Alberta; 2014.
12. 10.1115/1.326445210.1115/1.3264452 ↗
13. 10.1016/S1359-6454(97)00238-310.1016/S1359-6454(97)00238-3 ↗
14. 10.3390/ma1210172410.3390/ma12101724 ↗
15. 10.1179/026708310X52053810.1179/026708310X520538 ↗
16. Larson FR. · Trans ASME · 1952 · 74 · 765
17. Hertzberg RW. · J Mater Educ · 1997 · 19 · 227
18. Canale LC · Int J Microstruct Mater Prop · 2008 · 3 · 474
19. 10.1016/S0364-5916(02)00037-810.1016/S0364-5916(02)00037-8 ↗
20. 10.1002/352760264X.ch510.1002/352760264X.ch5 ↗
21. 10.1016/0022-3697(61)90054-310.1016/0022-3697(61)90054-3 ↗
22. Wagner C. · Z Elektrochem · 1961 · 65 · 581
23. 10.1007/s12613-017-1503-510.1007/s12613-017-1503-5 ↗
24. 10.1007/s11661-007-9403-310.1007/s11661-007-9403-3 ↗