journal article·1996-05

Behaviour of short cracks in alloy 800HT under biaxial fatigue

Z. Mu, H. Vehoff, M. Brede, P. Neumann

Materials Science and Technology· Volume 12· Issue 5
Publisher page

Abstract

Biaxial in phase fatigue tests were carried out on thin walled tube specimens of alloy 800HT at ambient temperature. The loading modes included tension, torsion, and combined tension—torsion with a tensile/shear plastic strain range ratio Δϵp/Δγp = 31/2. The influence of effective strain amplitudes and biaxiality on the initial growth of fatigue cracks was investigated using the replica technique. The results indicated that the loading conditions strongly affected the growth rates of short cracks. In torsion the cracks grew significantly more slowly than under axial or biaxial loading. A mean tensile stress perpendicular to the shear crack promoted its growth and reduced the fatigue life. The growth of the cracks could be described by the ΔJ integral for axial and biaxial loading; the integration predicted the fatigue life under axial and biaxial loading correctly. However, significantly conservative lifetime predictions were obtained for pure torsional loading since ΔJ does not include crack closure and crack surface rubbing.MST/3234
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Fatigue and fracture mechanics · High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. PARSONS M. W. · Proc. Inst. Mech. Eng. · 1975 · 188 · 61
2. 10.1111/j.1460-2695.1979.tb00379.x10.1111/j.1460-2695.1979.tb00379.x ↗
3. N. HAMADA, M. SAKANE, and M. OHNAMI: in Proc. 3rd Int. Conf. on ‘Biaxial/multiaxial fatigue’, Stuttgart, Germany, April 1989, Vol. 2, 41.1–41.15.
4. 10.1111/j.1460-2695.1984.tb00187.x10.1111/j.1460-2695.1984.tb00187.x ↗
5. D. F. SOCIE, L. A. WAILL, and D. F. DITTMER: in ‘Multiaxial fatigue’, STP 853, 468–481; 1984, Philadelphia, PA, ASTM.
6. H. HEITMANN, H. VEHOFF, and P. NEUMANN: in Proc. 6th Int. Conf. on Fracture, (ed. S. R. Valluri et al), Vol. 5, 3599–3606; 1984, Oxford, Pergamon Press.10.1016/B978-1-4832-8440-8.50388-4 ↗
7. J. PROCHOTTA and P. NEUMANN: in Proc. ECF8 ‘Fracture behaviour and design of materials and structures’, (ed. D. Firrao), Torino, Italy, October 1990, Vol.3, 1317–1322, European Group on Fracture.
8. DeLANGE R. G. · Trans. TMS-AIME · 1964 · 230 · 644
9. 10.1115/1.315774210.1115/1.3157742 ↗
10. N. J. HURT and P. E. IRVING: in ‘Design of fatigue and fracture resistant structures’, STP 761, 212–233; 1982, Philadelphia, PA, ASTM.10.1520/STP28861S ↗
11. 10.1520/STP23213S10.1520/STP23213S ↗