Abstract

This study details the development of microstructure of Ti14 alloy as a function of the forging temperature and forging ratio in semisolid state and influence of resulting microstructure on the mechanical properties. The results reveal that dynamic recrystallisation occurred during semisolid forging, and the grain refinement was attained. Grain size increased in the forging temperature and decreased in the forging ratio. High ultimate tensile strengths and low elongation have been achieved after semisolid forging. The strength decreased with increasing forging temperature, while the ductility increased with increasing forging ratio. The relative contributions of tensile properties were attributed to the varieties of grain size obtained by thixoforging.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Titanium Alloys Microstructure and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering Chang'an University, Xi'an 710064, China

State Key Laboratory for Mechanical Behavior of Materials Xi'an Jiaotong University, Xi'an 710049, China

References (19)

Show source-provided references
1. 10.1007/BF0265122710.1007/BF02651227 ↗
2. Kirwood D. H. · Int. Mater. Rev. · 1994 · 39 · 957
3. 10.1016/S0261-3069(97)00071-X10.1016/S0261-3069(97)00071-X ↗
4. 10.1016/S0079-6425(03)00037-910.1016/S0079-6425(03)00037-9 ↗
5. 10.1016/S0921-5093(04)00928-110.1016/S0921-5093(04)00928-1 ↗
6. 10.1016/j.msea.2008.07.02710.1016/j.msea.2008.07.027 ↗
7. 10.1016/S1359-6454(98)00356-510.1016/S1359-6454(98)00356-5 ↗
8. 10.1016/S1359-6454(99)00252-910.1016/S1359-6454(99)00252-9 ↗
9. 10.1016/j.scriptamat.2008.11.01110.1016/j.scriptamat.2008.11.011 ↗
10. 10.1016/j.actamat.2007.08.01010.1016/j.actamat.2007.08.010 ↗
11. 10.1007/978-3-540-71398-210.1007/978-3-540-71398-2 ↗
12. 10.1016/j.msea.2004.02.00510.1016/j.msea.2004.02.005 ↗
13. 10.1016/j.msea.2005.10.03810.1016/j.msea.2005.10.038 ↗
14. Zhao Y. Q.: Chinese patent no. 02101189·3.
15. 10.1023/A:100487350100510.1023/A:1004873501005 ↗
16. Mao W. M. ‘Recrystallization and grain growth of metal’, 242; 1993, Beijing, Metallurgical Industry Press.
17. 10.1016/S1359-6454(99)00045-210.1016/S1359-6454(99)00045-2 ↗
18. 10.1016/S1359-6454(03)00162-910.1016/S1359-6454(03)00162-9 ↗
19. 10.1016/1359-6454(96)00072-910.1016/1359-6454(96)00072-9 ↗