journal article·2021-05

Effects of extrusion speed and compounds on surface defects in extruded-AA7003 alloy

T. Homma, T. Honma, D. Terada, M. Hoshino

Materials Science and Technology· Volume 37· Issue 8
Publisher page

Abstract

The defect formation in a rod-shaped AA7003 alloy is carefully treated in the sample extruded at 10 or 20 m min −1 with their structure–property relationships. The <111> + <100> double fibre texture is formed in the extruded rods, but it is altered near the surface of the extrudates due to recrystallisation and recovery, being triggered by the processing heat. This reduces strains at the region, leading to softening of the hardness. Coarse Al 9 (Mn,Fe) 2 Si compounds are transported to the die throat with the fragmentation. The agglomeration of compounds occurs near the surface and makes pick-up. Eventually the number of pick-up is much higher in the sample extruded at 20 m min −1 .
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical Engineering, Nagaoka University of Technology, Nagaoka, Japan

Department of Mechanical Science and Engineering, Faculty of Engineering, Chiba Institute of Technology, Narashino, Japan

Department of Mechanical Engineering, College of Science and Technology, Nihon University, Chiyoda, Tokyo, Japan

Funding

Japan Institute of Light Metals · Light Metal Education Foundation

References (29)

Show source-provided references
1. 10.2464/jilm.24.2510.2464/jilm.24.25 ↗
2. Yoshida H. Alloy development for transportation in Sumitomo light metal. In: Proceedings of the 12th Int. Conf. Aluminium Alloys; Yokohama, Japan. The Jpn Inst Light Met; 2010. p. 54–61.
3. 10.2320/matertrans1960.11.40410.2320/matertrans1960.11.404 ↗
4. 10.2320/materia1962.17.49810.2320/materia1962.17.498 ↗
5. 10.1179/mtlr.1971.16.1.9510.1179/mtlr.1971.16.1.95 ↗
6. 10.2320/matertrans1960.7.22410.2320/matertrans1960.7.224 ↗
7. 10.1007/978-1-4757-3001-210.1007/978-1-4757-3001-2 ↗
8. Polmear I · 2017
9. 10.1016/j.jmatprotec.2006.11.17710.1016/j.jmatprotec.2006.11.177 ↗
10. 10.2464/jilm.44.68210.2464/jilm.44.682 ↗
11. 10.2978/jsas.13.30910.2978/jsas.13.309 ↗
12. 10.1016/S0890-6955(01)00148-110.1016/S0890-6955(01)00148-1 ↗
13. 10.1016/j.jmatprotec.2006.04.09810.1016/j.jmatprotec.2006.04.098 ↗
14. 10.1179/mst.1990.6.8.75510.1179/mst.1990.6.8.755 ↗
15. 10.1179/02670830422502201610.1179/026708304225022016 ↗
16. Bryand AJ. · Z Metallkde · 1971 · 62 · 701
17. Parson NC, Jowett CW, Fraser WC Surface defects on 6XXX alloy extrusions. In: Proceedings of 6th Int. Aluminum Extrusion Tech. Seminar; May 14–17. Vol. 1. Aluminum Association; 1996. p. 57–67.
18. 10.2464/jilm.49.25310.2464/jilm.49.253 ↗
19. 10.1017/S143192761100005510.1017/S1431927611000055 ↗
20. 10.2320/matertrans1960.5.23510.2320/matertrans1960.5.235 ↗
21. 10.2464/jilm.17.310.2464/jilm.17.3 ↗
22. 10.1016/j.ultramic.2011.02.00410.1016/j.ultramic.2011.02.004 ↗
23. Villars P · 1991
24. 10.1107/S0365110X6600149X10.1107/S0365110X6600149X ↗
25. 10.1107/S160057671700937210.1107/S1600576717009372 ↗
26. 10.1080/1478643700823842610.1080/14786437008238426 ↗
27. 10.1155/TSM.1.23310.1155/TSM.1.233 ↗
28. 10.1016/B978-008044164-1/50008-610.1016/B978-008044164-1/50008-6 ↗
29. 10.1016/j.msea.2018.05.10510.1016/j.msea.2018.05.105 ↗