Ni–43Ti–7Al (at-) alloy was directionally solidified at different withdrawal rates (2, 20 and 100 μm s−1) and a constant temperature of 1550°C by liquid metal cooling method. Results show that as the withdrawal rate decreases from 100 to 2 μm s−1, the cellular arm spacing increases from 39·5 to 126 μm, the size of Ti2Ni and the stability of the liquid/solid interface also increase, while the volume fraction of Ti2Ni decreases from 3·1 to 0·9. Moreover, microstructural analysis reveals that a NiTi+Ti2Ni anomalous eutectic structure is formed in intercellular regions of directionally solidified samples withdrawn at 20 and 100 μm s−1. However, in the sample withdrawn at 2 μm s−1, Ti2Ni phases represent strip and liquid droplet morphologies in the intercellular region. Finally, the possible explanation to the change of microstructure is discussed.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Shape Memory Alloy Transformations · Metallic Glasses and Amorphous Alloys · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Key Laboratory of Aerospace Advanced Materials and Performance of Ministry of Education School of Materials Science and Engineering, Beihang University, Beijing 100191, China
References (27)
Show source-provided references
1. Otsuka K, Wayman CM: ‘Shape memory materials’, 1; 1998, London, Cambridge University Press.
2. 10.1016/B978-0-7506-1009-4.50015-910.1016/B978-0-7506-1009-4.50015-9 ↗
3. 10.1016/S0921-5093(96)10508-610.1016/S0921-5093(96)10508-6 ↗
4. 10.1016/S0921-5093(96)10472-X10.1016/S0921-5093(96)10472-X ↗
5. Meng LJ: ‘Study of NiTi–Al based high temperature structural materials’, PhD thesis, Beihang University, Beijing, China, 2006.
6. 10.1016/j.intermet.2006.10.03810.1016/j.intermet.2006.10.038 ↗
7. 10.1134/S003602950705010210.1134/S0036029507050102 ↗
8. 10.1002/adem.20050025810.1002/adem.200500258 ↗
9. Nevitt MV · Trans. Metall. Soc. AIME · 1960 · 218 · 327
10. 10.1016/0925-8388(94)90079-510.1016/0925-8388(94)90079-5 ↗
11. Zhou L
12. 10.1016/j.actamat.2010.02.01910.1016/j.actamat.2010.02.019 ↗
13. 10.3724/SP.J.1037.2010.0089010.3724/SP.J.1037.2010.00890 ↗
14. Murray JL: ‘The Ti–Ni system, phase diagrams of binary titanium alloys’, 197; 1987, Materials Park, OH, ASM International.
15. 10.2320/matertrans1989.39.62310.2320/matertrans1989.39.623 ↗
16. 10.1016/j.jallcom.2009.05.07810.1016/j.jallcom.2009.05.078 ↗
17. 10.1016/S0966-9795(02)00131-010.1016/S0966-9795(02)00131-0 ↗
18. 10.4028/www.scientific.net/MSF.307.2510.4028/www.scientific.net/MSF.307.25 ↗
19. 10.1016/0956-7151(94)90289-510.1016/0956-7151(94)90289-5 ↗
20. 10.1016/j.jmatprotec.2005.02.17710.1016/j.jmatprotec.2005.02.177 ↗
21. 10.1016/j.jallcom.2009.02.05610.1016/j.jallcom.2009.02.056 ↗
22. 10.1557/JMR.1987.080910.1557/JMR.1987.0809 ↗
23. 10.1016/j.jcrysgro.2004.07.03110.1016/j.jcrysgro.2004.07.031 ↗
24. 10.1016/0921-5093(94)90558-410.1016/0921-5093(94)90558-4 ↗
25. Nagasgio K · Scr. Mater. · 1999 · 41 · 116110.1016/S1359-6462(99)00286-9 ↗
26. Hillert M: ‘Solidification and casting of metals’, 81; 1979, London, The Metals Society Press.
27. 10.1557/PROC-19-22310.1557/PROC-19-223 ↗