journal article·2012-11

Influence of chemistry on transverse cracking during continuous casting of medium C high N steel billets

K M Banks, A S Tuling, B Mintz

Materials Science and Technology· Volume 28· Issue 11
Publisher page

Abstract

Corner cracking in medium C electric arc steel was experienced after continuous casting of square billets. This led to the investigation of the influence of high N levels on hot ductility. Steels microalloyed with V, Ti and B were subjected to in situ melting followed by cooling according to typical off-corner temperature profiles. Steels containing moderate amounts of V resulted in good ductility at the estimated off-corner temperature during unbending of 900°C due to the suppression of precipitation. Ti additions to V, Al, Si and B containing steels, although beneficial at low N levels, are detrimental to hot ductility when the N content is high due to a higher precipitate volume fraction. High Ti–B steels produced the worst hot ductility in medium C steels containing high N.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metallurgical Processes and Thermodynamics · Magnetic Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

IMMRI, University of Pretoria, Pretoria, South Africa

City UniversityLondon, UK

References (20)

Show source-provided references
1. 10.1179/095066009X1257253017062410.1179/095066009X12572530170624 ↗
2. Banks KM · SAIMM · 2011 · 111 · 711
3. 10.1142/S021797920906056710.1142/S0217979209060567 ↗
4. 10.4028/www.scientific.net/MSF.500-501.16310.4028/www.scientific.net/MSF.500-501.163 ↗
5. M. W. Erwee and P. C. Pistorius: Ironmaking Steelmaking, 2012, 39, (5), 336–341.10.1179/1743281211Y.0000000076 ↗
6. Mintz B · Ironmaking Steelmaking · 2012 · 39 · 33610.1179/1743281211Y.0000000076 ↗
7. 10.1179/026708309X1258456405213910.1179/026708309X12584564052139 ↗
8. 10.1179/1743284711Y.000000009410.1179/1743284711Y.0000000094 ↗
9. 10.1179/mst.1996.12.6.45310.1179/mst.1996.12.6.453 ↗
10. 10.1007/BF0265843710.1007/BF02658437 ↗
11. Wang B · J. Iron Steel Res. · 2008 · 15 · 1610.1016/S1006-706X(08)60137-5 ↗
12. ArcelorMittal R&D: private communication, 2011.
13. 10.1179/imr.1988.33.1.22110.1179/imr.1988.33.1.221 ↗
14. 10.2355/isijinternational1966.25.14910.2355/isijinternational1966.25.149 ↗
15. Yamamoto K, Suzuki HG, Oono Y, Noda N, Inoue T: ‘Formation mechanism and prevention methods for facial cracks in continuously cast steel slabs containing boron’, Nippon Steel, Tokyo, Japan, 1985.
16. Cho KC · Metall. Mater. Trans. A · 2010 · 41 · 1422
17. 10.1179/02670839910150584210.1179/026708399101505842 ↗
18. Bouet M, Root J, Es-sadiqui E, Yue S: Proc. 40th MWSP Conf., Pittsburgh, PA, USA, November 1988, ISS, 675–684.
19. Chamont B, Chenelle P, Blausser H: Proc. Conf. on ‘Physical simulation techniques for welding, hot forming and continuous casting’, Ottawa, Ont., Canada, May 1988, MTL, CANMET, 11–48.
20. 10.1179/mst.1991.7.12.110110.1179/mst.1991.7.12.1101 ↗