Thermal fatigue resistance of H13 die steel repaired by partial laser surface remelting process
Source abstract
Abstract
In order to study the thermal fatigue resistance of H13 die steel repaired by a partial laser surface remelting process, a strengthening latticed morphology was designed and processed using a pulsed Nd:YAG laser by imitating the structures of certain animals and plants. The ultrafine microstructure within the strengthening unit is composed of martensite, austenite and finer carbides. The average microhardness of the unit is much higher than that of the original surface, even after thermal fatigue cycles. The results show that both percentage increase in crack length and crack density are reduced owing to the blocking effect of strengthening units. Partial laser surface remelting with the smallest spacing is the most effective for repairing cracks and improving the overall thermal fatigue resistance. A manufacturing verification test demonstrates the effectiveness of the partial laser remelting process in repairing thermal fatigue cracks of a casting die and improving its thermal fatigue resistance.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: High Entropy Alloys Studies · Additive Manufacturing Materials and Processes · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
The Key Lab of Automobile Materials, The Ministry of Education, Jilin University, Changchun 130025, China
The Key Lab of Terrain Machinery Bionics Engineering, The Ministry of Education, Jilin University, Changchun 130025, China
FAW Foundry Co. Ltd, First Automobile Works Group Corporation, Changchun 130011, China
References (32)
Show source-provided references
1. 10.1016/S0257-8972(00)01075-610.1016/S0257-8972(00)01075-6 ↗
2. 10.1016/j.surfcoat.2004.04.05310.1016/j.surfcoat.2004.04.053 ↗
3. 10.1016/j.commatsci.2008.03.00910.1016/j.commatsci.2008.03.009 ↗
4. 10.1016/j.engfailanal.2011.11.00610.1016/j.engfailanal.2011.11.006 ↗
5. Muhič M. · Metalurgija · 2010 · 49 · 9
6. 10.1016/j.surfcoat.2006.09.05110.1016/j.surfcoat.2006.09.051 ↗
7. 10.1016/j.jmatprotec.2012.07.01810.1016/j.jmatprotec.2012.07.018 ↗
8. 10.1007/s11666-007-9028-510.1007/s11666-007-9028-5 ↗
9. 10.1016/S0921-5093(02)00477-X10.1016/S0921-5093(02)00477-X ↗
10. 10.1016/j.surfcoat.2012.09.03910.1016/j.surfcoat.2012.09.039 ↗
11. Burakowski T., and Wierzchon T. ‘Surface engineering of metals: principles, equipment, technologies’; 2010, New York, CRC Press.
12. 10.1007/s12289-010-0890-110.1007/s12289-010-0890-1 ↗
13. 10.1016/j.apsusc.2007.09.10210.1016/j.apsusc.2007.09.102 ↗
14. 10.1016/S1672-6529(10)60271-510.1016/S1672-6529(10)60271-5 ↗
15. 10.1006/jaer.2001.072210.1006/jaer.2001.0722 ↗
16. 10.1016/S0022-4898(03)00012-010.1016/S0022-4898(03)00012-0 ↗
17. 10.1016/j.matdes.2010.07.01910.1016/j.matdes.2010.07.019 ↗
18. 10.1016/j.surfcoat.2005.10.01910.1016/j.surfcoat.2005.10.019 ↗
19. 10.1179/1743284712Y.000000016910.1179/1743284712Y.0000000169 ↗
20. 10.1016/S1672-6529(08)60069-410.1016/S1672-6529(08)60069-4 ↗
21. 10.1016/j.jmatprotec.2007.07.03310.1016/j.jmatprotec.2007.07.033 ↗
22. 10.1016/j.optlastec.2013.04.02410.1016/j.optlastec.2013.04.024 ↗
23. 10.1016/j.ijfatigue.2005.06.04210.1016/j.ijfatigue.2005.06.042 ↗
24. 10.1016/S0921-5093(97)00507-810.1016/S0921-5093(97)00507-8 ↗
25. 10.1016/j.scriptamat.2010.06.03010.1016/j.scriptamat.2010.06.030 ↗
26. 10.1016/j.apsusc.2007.05.00810.1016/j.apsusc.2007.05.008 ↗
27. 10.1016/j.matlet.2005.02.02610.1016/j.matlet.2005.02.026 ↗
28. Zhang Z. · 2013
29. 10.1017/CBO978051180657510.1017/CBO9780511806575 ↗
30. 10.1023/A:101865591705110.1023/A:1018655917051 ↗
31. 10.1179/mst.1994.10.3.20910.1179/mst.1994.10.3.209 ↗
32. 10.1016/S0142-1123(97)00113-810.1016/S0142-1123(97)00113-8 ↗