The bond shear test was used to assess the integrity of Sn–0·7Cu and Sn–0·3Ag–0·7Cu lead-free solder alloy drops solidified on copper substrates with smooth and rough surface finishes. Solder alloys solidified on smooth substrates required higher shear force compared to that on rough substrates. Sn–0·3Ag–0·7Cu alloy required higher shear energy than Sn–0·7Cu alloy. Solder alloys solidified on smooth substrate surfaces exhibited complete ductile failure. On rough copper surfaces, solder alloys showed a transition ridge characterized by sheared intermetallic compounds (IMCs) and the presence of dimples. The peak shear strength decreased with increase in contact area of the solder bond on the substrate. Smooth surface and the presence of minor amount of Ag in the solder alloy enhance the integrity of the solder joint.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Advanced Welding Techniques Analysis · 3D IC and TSV technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Metallurgical & Materials Engineering, National Institute of Technology Karnataka, Surathkal, Mangalore 575 025, Karnataka, India

References (18)

Show source-provided references
1. Hwang JS: ‘Implementing lead-free electronics’, 1–40; 2005, New York, McGraw-Hill.
2. 10.1201/9780849391088.ax310.1201/9780849391088.ax3 ↗
3. Sweatman K, Suenaga S, Nishimura T: Proceedings Pan Pacific, 127–133; 2008, SMTA.
4. 10.1007/s10854-011-0291-310.1007/s10854-011-0291-3 ↗
5. 10.1016/j.jallcom.2011.01.06210.1016/j.jallcom.2011.01.062 ↗
6. 10.1007/s10853-010-5231-810.1007/s10853-010-5231-8 ↗
7. Liu X, Wang L, Wang J, Lv Y: ‘11th International Conference on Electronic Packaging Technology & High Density Packaging’, 2010, 176–180.
8. 10.1016/S1005-0302(12)60023-110.1016/S1005-0302(12)60023-1 ↗
9. 10.1016/j.mser.2005.03.00110.1016/j.mser.2005.03.001 ↗
10. Huang X, Lee SWR, Yan CC, Hui S: ‘Proceedings of the 2001 Electronic Components and Technology Conference. IEEE’, Orlando, 1065–1071, IEEE.
11. Huang X., Lee S.W.R., Yan C.C., Hui S. ‘Proceedings of the 2002 Electronic Components and Technology Conference. IEEE’, San Diego, 968–973, 2002, IEEE.
12. 10.1016/j.msea.2003.12.01210.1016/j.msea.2003.12.012 ↗
13. 10.1016/j.jallcom.2004.05.00910.1016/j.jallcom.2004.05.009 ↗
14. 10.1016/j.ijsolstr.2005.07.01410.1016/j.ijsolstr.2005.07.014 ↗
15. 10.1007/s10854-012-0644-610.1007/s10854-012-0644-6 ↗
16. 10.2320/matertrans.42.73910.2320/matertrans.42.739 ↗
17. 10.1016/j.microrel.2008.07.06610.1016/j.microrel.2008.07.066 ↗
18. 10.1007/s11664-004-0086-x10.1007/s11664-004-0086-x ↗