journal article·2016-09

Role of MgO nanoparticles on zirconia-toughened alumina-5 wt-% CeO 2 ceramics mechanical properties

N. A. Rejab, A. Z. Ahmad Azhar, M. M. Ratnam, Z. A. Ahmad

Materials Science and Technology· Volume 32· Issue 13
Publisher page

Abstract

The poor hardness of zirconia-toughened alumina (ZTA) with 5 wt-% CeO 2 (ZTA5CeO 2 ) ceramic has limited its applications as a cutting insert. Therefore, in this work, the possibility of MgO nanoparticles (20 nm) as reinforcement to ZTA5CeO 2 ceramics was investigated. Mgo nanoparticles with different weight percentages (0-2 wt-%) were added to ZTA5CeO 2 ceramics. ZTA5CeO 2 with 0.5 wt-%MgO showed the highest fracture toughness of 9.14 MPa.√m. The addition of 0.5 wt-%MgO nanoparticles showed the excellent role of MgAl 11 CeO 19 grains as a crack deflector, which consequently produced a reasonable hardness value of 1591 HV and lowered the wear areas to 0.0528 mm 2 .
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Structural Materials Niche Area, School of Materials and Mineral Resources Engineering, Engineering Campus, Universiti Sains Malaysia, 14300 Nibong Tebal, Penang, Malaysia

Department of Manufacturing and Materials Engineering, Faculty of Engineering, International Islamic University Malaysia, 50728 Gombak, Selangor, Malaysia

School of Mechanical Engineering, Engineering Campus, Universiti Sains Malaysia, 14300 Nibong Tebal, Penang, Malaysia

Funding

Universiti Sains Malaysia

References (27)

Show source-provided references
1. 10.1016/j.ijrmhm.2015.01.00510.1016/j.ijrmhm.2015.01.005 ↗
2. 10.1016/j.jallcom.2011.09.09210.1016/j.jallcom.2011.09.092 ↗
3. 10.1016/j.ijrmhm.2011.02.00210.1016/j.ijrmhm.2011.02.002 ↗
4. 10.1016/j.jallcom.2010.03.05410.1016/j.jallcom.2010.03.054 ↗
5. Azhar A. Z. A. Rejab N. A. Hasmaliza M. Ratnam M. M. and Zainal A. A.: ‘The effects of Cr2O3 addition on fracture toughness and phases of ZTA ceramic composite’ Adv. Mater. Res. 2012b 620 35–39 doi:10.4028/www.scientific.net/AMR.620.35.10.4028/www.scientific.net/AMR.620.35 ↗
6. 10.1016/S0142-9612(01)00206-X10.1016/S0142-9612(01)00206-X ↗
7. 10.1016/j.ceramint.2012.08.06510.1016/j.ceramint.2012.08.065 ↗
8. 10.1179/02670838779022095510.1179/026708387790220955 ↗
9. 10.1016/j.ceramint.2014.07.02710.1016/j.ceramint.2014.07.027 ↗
10. 10.1179/174328408X38973310.1179/174328408X389733 ↗
11. 10.1007/BF0036686910.1007/BF00366869 ↗
12. 10.1016/S0955-2219(01)00528-310.1016/S0955-2219(01)00528-3 ↗
13. 10.1016/S0079-6425(00)00005-010.1016/S0079-6425(00)00005-0 ↗
14. 10.1016/j.ceramint.2011.11.06210.1016/j.ceramint.2011.11.062 ↗
15. 10.1016/j.ijrmhm.2010.12.00110.1016/j.ijrmhm.2010.12.001 ↗
16. 10.1016/j.ceramint.2014.11.08010.1016/j.ceramint.2014.11.080 ↗
17. 10.1016/S0272-8842(97)00048-510.1016/S0272-8842(97)00048-5 ↗
18. 10.1007/BF0072562510.1007/BF00725625 ↗
19. 10.1134/S002016851303016310.1134/S0020168513030163 ↗
20. 10.1016/j.msea.2013.11.09110.1016/j.msea.2013.11.091 ↗
21. 10.1016/j.ijrmhm.2012.08.01010.1016/j.ijrmhm.2012.08.010 ↗
22. 10.1007/s00170-007-1119-410.1007/s00170-007-1119-4 ↗
23. 10.1016/j.ceramint.2013.11.07610.1016/j.ceramint.2013.11.076 ↗
24. 10.1016/j.ceramint.2012.01.05110.1016/j.ceramint.2012.01.051 ↗
25. 10.1007/BF0238572110.1007/BF02385721 ↗
26. 10.1016/j.ceramint.2007.06.00510.1016/j.ceramint.2007.06.005 ↗
27. 10.1179/174328408X28768210.1179/174328408X287682 ↗