journal article·2014-12

On effect of salt deposits on oxidation behaviour of CMSX-4 above 1000°C

S. Pahlavanyali, H. T. Pang, F. Li, S. Bagnall, C. Rae

Materials Science and Technology· Volume 30· Issue 15
Publisher page

Abstract

Whereas the effect of contaminants in causing hot corrosion has been extensively studied at temperatures up to 1000°C, this paper describes a systematic study of the effects of various salt deposits on the cyclic oxidation of CMSX-4** in air at temperatures above 1000°C. The alloy was tested both in the bare and in the platinum aluminised (Pt-Al) coated conditions and variables included temperature, salt concentration, and sulphur level of the original alloy. It was found that salt deposition at very moderate levels, re-applied at regular intervals, significantly increased the initial weight gain and decreased the time to first spallation despite the rapid loss of the salt through evaporation in the first heating up cycle subsequent to salt deposition. The degraded microstructure of the specimens tested with salt resembled closely that of blades having experienced engine service conditions. Hence, cyclic oxidation with the addition of salt offers an accurate, flexible, reproducible and above all realistic method of assessing the life of turbine components.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · nanoparticles nucleation surface interactions · Catalytic Processes in Materials Science

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

ERA Technology Ltd., Cleeve Road, Leatherhead KT22 7SA, UK

Department of Materials Science and Metallurgy, University of Cambridge, 27 Charles Babbage Road, Cambridge CB3 0FS, UK

Rolls-Royce plc., PO Box 31, Derby DE24 8BJ, UK

References (22)

Show source-provided references
1. 10.1017/CBO978113916390310.1017/CBO9781139163903 ↗
2. 10.1017/CBO978051154128510.1017/CBO9780511541285 ↗
3. Young DJ: ‘High temperature oxidation and corrosion of metals’; 2008, Amsterdam, Elsevier Science.
4. 10.1007/BF0066691310.1007/BF00666913 ↗
5. 10.1149/1.240783710.1149/1.2407837 ↗
6. 10.1007/BF0060654410.1007/BF00606544 ↗
7. 10.1179/imr.1995.40.1.110.1179/imr.1995.40.1.1 ↗
8. 10.1016/0040-6090(94)90335-210.1016/0040-6090(94)90335-2 ↗
9. 10.1007/BF0264962610.1007/BF02649626 ↗
10. 10.1016/S0010-938X(01)00057-910.1016/S0010-938X(01)00057-9 ↗
11. 10.1016/S0257-8972(99)00343-610.1016/S0257-8972(99)00343-6 ↗
12. 10.1007/s11661-999-0128-310.1007/s11661-999-0128-3 ↗
13. 10.1007/s11085-007-9067-910.1007/s11085-007-9067-9 ↗
14. 10.1007/BF0108078410.1007/BF01080784 ↗
15. Smialek JL: ‘Cyclic oxidation modeling and life prediction’, 663–670; 2004, Materials Science Forum.10.4028/www.scientific.net/MSF.461-464.663 ↗
16. 10.1016/j.surfcoat.2006.07.25610.1016/j.surfcoat.2006.07.256 ↗
17. 10.1016/0040-6090(82)90019-010.1016/0040-6090(82)90019-0 ↗
18. 10.1007/BF0283336110.1007/BF02833361 ↗
19. 10.1002/adem.20080001510.1002/adem.200800015 ↗
20. ASTM E1019-11: ‘Standard test methods for determination of carbon, sulfur, nitrogen, and oxygen in steel, iron, nickel, and cobalt alloys by various combustion and fusion techniques’; 2011, West Conshohocken, ASTM.
21. 10.1115/1.281813210.1115/1.2818132 ↗
22. 10.1179/174327807X15992510.1179/174327807X159925 ↗