Influence of sintering on bending strength of underwater shock consolidated Al–SiCp composites
Source abstract
Abstract
Aluminium matrix composites containing 10, 20 and 30 vol.-%SiC particles were manufactured with underwater shock consolidation method. Sintering of the compact specimens was carried out at 400°C for 70 min. Density, hardness and bending strength of the specimens were measured before and after sintering treatment. SEM fractography examination was used for analysis of fracture surfaces of the consolidated specimens. The sintered specimens with 10 vol.-%SiCp showed enhancement in the bending strength and deflection. After sintering, the fracture surface of 10 vol.-%SiCp composite showed cleaved SiC particles, indicating appreciable improvement in bonding strength between ceramic reinforcement particle and Al matrix.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis · High-Velocity Impact and Material Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Noguchi M., and Takahashi K.: Key Eng. Mater., 1997, 127-131,153–164.10.4028/www.scientific.net/KEM.127-131.153 ↗
2. Maruyama B. · Adv. Mater. Process · 1998 · 3 · 6
3. 10.1007/BF0113373910.1007/BF01133739 ↗
4. 10.1179/pom.1989.32.1.5310.1179/pom.1989.32.1.53 ↗
5. 10.1111/j.1151-2916.1978.tb09290.x10.1111/j.1151-2916.1978.tb09290.x ↗
6. Prummer R. A. · Powder Metall Int · 1985 · 9 · 1035
7. Thadani N. N. · Adv. Mater. Manuf Process · 1988 · 3 · 49
8. 10.1146/annurev.ms.16.080186.00153110.1146/annurev.ms.16.080186.001531 ↗
9. 10.1007/BF0266941410.1007/BF02669414 ↗
10. 10.1016/S0924-0136(98)00273-810.1016/S0924-0136(98)00273-8 ↗
11. 10.1016/S0924-0136(98)00272-610.1016/S0924-0136(98)00272-6 ↗
12. 10.1016/S0925-9635(00)00581-110.1016/S0925-9635(00)00581-1 ↗
13. 10.1016/S0921-4526(97)00368-210.1016/S0921-4526(97)00368-2 ↗
14. 10.1016/S0921-4526(97)00364-510.1016/S0921-4526(97)00364-5 ↗
15. 10.1016/S0924-0136(98)00270-210.1016/S0924-0136(98)00270-2 ↗
16. 10.1016/S0924-0136(02)01117-210.1016/S0924-0136(02)01117-2 ↗
17. 10.1016/S0924-0136(98)00271-410.1016/S0924-0136(98)00271-4 ↗
18. 10.1016/S1359-6462(98)00311-X10.1016/S1359-6462(98)00311-X ↗
19. 10.1016/S0734-743X(99)00034-210.1016/S0734-743X(99)00034-2 ↗
20. 10.1023/A:102007141606310.1023/A:1020071416063 ↗
21. Kumar K. S. · Int. J. Powder Metall · 1992 · 28 · 63
22. 10.1016/S0924-0136(97)00237-910.1016/S0924-0136(97)00237-9 ↗
23. 10.1080/10667857.1996.1175269810.1080/10667857.1996.11752698 ↗
24. 10.1023/A:102673992097610.1023/A:1026739920976 ↗
25. 10.1016/S0924-0136(01)00559-310.1016/S0924-0136(01)00559-3 ↗
26. Kumar K. S., Hokamoto K., Nakano S., and Fujita M.: Proc. EXPLOMET 2000, (ed.Staudhammer K. P.), 313-320; 2001, New York, Elsevier.
27. Hokamoto K., Raghukandan K., Lee J. S., Fujita M., and Tomoshige R.: Mater. Set Forum, 2003, 437-438,169–172.10.4028/www.scientific.net/MSF.437-438.169 ↗
28. Eskandari H., Hokamoto K., Ghasemi H. M., and Emamy M., Borji S., Lee J. S.: Mater. Sci. Forum, 2004, 465-466, 433.10.4028/www.scientific.net/MSF.465-466.433 ↗
29. Itoh S. · J. Jpn Explos. Soc · 1994 · 55 · 71
30. Eskandari H., Ghasemi H. M., and Emamy M.: Mater. Sci. Forum, 2004, 465-466, 213.10.4028/www.scientific.net/MSF.465-466.213 ↗
31. Gupta M. · Aluminum Trans · 1999 · 1 · 33
32. Li Y. · Mater. Sci. Eng. A · 2004 · 371 · 366
33. 10.1007/BF0281167910.1007/BF02811679 ↗
34. 10.1179/02670839379017142110.1179/026708393790171421 ↗