journal article·2012-06

Effect of Ni on growing of intermetallic compound in interface of Sn2·5Ag0·7Cu0·1RE/Cu solder joint during aging

K K Zhang, C Y Li, R F Qiu, H X Shi, Y L Wang

Materials Science and Technology· Volume 28· Issue 6
Publisher page

Abstract

Aging treatment was implemented for the Sn2·5Ag0·7Cu0·1RExNi/Cu solder joint under various temperatures simulating the service environment. The growing behaviour of the intermetallic compound at the soldering interface during aging was investigated. In the case of adding 0·1Ni aged solder joint, the maximum growth activation energies of (Cu,Ni)6Sn5 and Cu3Sn are 86·8 and 93·7 kJ mol−1 respectively. The results reveal that the growth of intermetallic compound in the soldering interface can be suppressed, and the solder joint can be strengthened by adding proper quantities of Ni in the solder.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

School of Materials Science and Engineering Henan University of Science and Technology, Luoyang 471003, China

Henan Key Laboratory of Science and Processing Technology of Non-ferrous Metals Henan University of Science and Technology, Luoyang 471003, China

References (17)

Show source-provided references
1. 10.1016/j.jallcom.2008.02.10210.1016/j.jallcom.2008.02.102 ↗
2. 10.1007/s10854-008-9732-z10.1007/s10854-008-9732-z ↗
3. 10.1007/s10854-010-0131-x10.1007/s10854-010-0131-x ↗
4. 10.1016/j.actamat.2007.09.02610.1016/j.actamat.2007.09.026 ↗
5. 10.4028/www.scientific.net/KEM.353-358.291210.4028/www.scientific.net/KEM.353-358.2912 ↗
6. 10.4028/www.scientific.net/MSF.650.9110.4028/www.scientific.net/MSF.650.91 ↗
7. 10.1016/S0026-2714(02)00239-110.1016/S0026-2714(02)00239-1 ↗
8. Wang L. F. · Transactions of the China Welding Institution. · 2009 · 30 · 9
9. 10.1016/S1003-6326(07)60157-510.1016/S1003-6326(07)60157-5 ↗
10. 10.1016/j.jallcom.2009.06.17110.1016/j.jallcom.2009.06.171 ↗
11. Ren HL: ‘Metallographic experiment technology’; 1986, Beijing, Metallurgical Industry Press.
12. 10.1007/s11664-006-0028-x10.1007/s11664-006-0028-x ↗
13. 10.1016/j.jallcom.2006.11.03610.1016/j.jallcom.2006.11.036 ↗
14. 10.1016/S1359-6454(01)00146-X10.1016/S1359-6454(01)00146-X ↗
15. 10.1016/j.microrel.2008.08.00710.1016/j.microrel.2008.08.007 ↗
16. 10.1016/j.jallcom.2009.06.15910.1016/j.jallcom.2009.06.159 ↗
17. 10.1007/BF0265334310.1007/BF02653343 ↗