Effects of cooling process on microstructure and hardness for 1·0C–1·5Cr bearing steel
Source abstract
Abstract
Effects of cooling rate ( Vcr) and final cooling temperature ( Tft), after hot deformation, on microstructure and hardness for 1·0C–1·5Cr bearing steel were investigated. The results show that if Vcr increases from 2 to 25°C s−1 and Tft remains at 650°C, pearlite colony size and grain size both decrease, hardness increases. When Vcr exceeds 8°C s−1, carbide network can be restrained effectively. TEM micrographs indicate that there exist branches in the local region of lamellar cementite and ferrite, and a ferrite thin film is also found around the proeutectoid carbide. Under the cooling rate of 10°C s−1, with the increase in Tft, the microstructure changes from martensite into pearlite, carbide network becomes more serious and hardness decreases.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
Fushun Special Steel Co., Ltd, Fushun 113001, China
References (28)
Show source-provided references
1. 10.1179/1743284711Y.000000004310.1179/1743284711Y.0000000043 ↗
2. 10.1179/1743284711Y.000000004710.1179/1743284711Y.0000000047 ↗
3. 10.1179/1743284711Y.000000006610.1179/1743284711Y.0000000066 ↗
4. 10.1016/S0921-5093(01)01436-810.1016/S0921-5093(01)01436-8 ↗
5. 10.1016/j.pmatsci.2011.06.00210.1016/j.pmatsci.2011.06.002 ↗
6. 10.1007/BF0283322410.1007/BF02833224 ↗
7. 10.1016/j.msea.2005.05.05110.1016/j.msea.2005.05.051 ↗
8. 10.1016/S0921-5093(01)01916-510.1016/S0921-5093(01)01916-5 ↗
9. 10.1179/026708310X1267799366208710.1179/026708310X12677993662087 ↗
10. 10.1179/02670839910150555410.1179/026708399101505554 ↗
11. 10.1179/02670830112500035710.1179/026708301125000357 ↗
12. 10.1179/026708310X1269949846300210.1179/026708310X12699498463002 ↗
13. 10.1179/mst.1995.11.6.56610.1179/mst.1995.11.6.566 ↗
14. 10.1016/S1644-9665(12)60207-610.1016/S1644-9665(12)60207-6 ↗
15. 10.1016/S1006-706X(10)60012-X10.1016/S1006-706X(10)60012-X ↗
16. ‘High-carbon chromium bearing steel’, GB/T 18254-2002, China.
17. 10.1016/j.matchar.2013.04.00710.1016/j.matchar.2013.04.007 ↗
18. 10.1016/j.matchar.2009.01.00110.1016/j.matchar.2009.01.001 ↗
19. 10.1007/BF0316182510.1007/BF03161825 ↗
20. 10.1016/j.actamat.2010.05.02310.1016/j.actamat.2010.05.023 ↗
21. 10.1016/S1044-5803(00)00055-310.1016/S1044-5803(00)00055-3 ↗
22. 10.1016/S1359-6454(02)00231-810.1016/S1359-6454(02)00231-8 ↗
23. 10.1016/0001-6160(56)90041-410.1016/0001-6160(56)90041-4 ↗
24. 10.1016/j.scriptamat.2012.03.01910.1016/j.scriptamat.2012.03.019 ↗
25. 10.1016/0956-7151(91)90002-I10.1016/0956-7151(91)90002-I ↗
26. 10.1016/j.matdes.2013.10.06210.1016/j.matdes.2013.10.062 ↗
27. 10.1016/S1044-5803(00)00056-510.1016/S1044-5803(00)00056-5 ↗
28. 10.1179/1743284713Y.000000049110.1179/1743284713Y.0000000491 ↗