The influences of deformation degrees on the microstructure evolution of GCr15 steel in cold ring rolling and following heat treatment (quenching and temper) are investigated in this paper. As the deformation is uneven, microstructure at the outer surface, middle place and inner surface on the cross-section of the ring is selected for the study. The microstructure is characterised by scanning electron microscopy, optical microscopy and X-ray diffraction. The [Formula: see text] transformation is studied with differential scanning calorimetry, and the hardness is examined by Vickers hardness tester. The results show that the deformation is severe on the outer surface but slight on the middle place and inner surface. A large degree of deformation leads to the acceleration of carbide dissolution, the grain refinement and the increase of hardness. In addition, the deformation results in the decrease of [Formula: see text] transformation temperature according to the differential scanning calorimetry data.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metallurgy and Material Forming · Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Hubei Key Laboratory of Advanced Technology for Automotive Components, Wuhan University of Technology 430070, Wuhan, China
Funding
the Innovative Research Team Development Program of Ministry of Education of China · the National Natural Science Foundation of China · Important Science and Technology Innovation Program of HuBei province · the Fundamental Research Funds for the Central Universities
References (21)
Show source-provided references
1. 10.1179/1743284713Y.000000049110.1179/1743284713Y.0000000491 ↗
2. 10.1179/1743284715Y.000000011310.1179/1743284715Y.0000000113 ↗
3. 10.1016/S0924-0136(97)00029-010.1016/S0924-0136(97)00029-0 ↗
4. 10.1016/j.jmatprotec.2006.11.03910.1016/j.jmatprotec.2006.11.039 ↗
5. 10.1016/j.ijmachtools.2007.01.00910.1016/j.ijmachtools.2007.01.009 ↗
6. 10.1016/S0924-0136(02)00354-010.1016/S0924-0136(02)00354-0 ↗
7. 10.1016/S0924-0136(03)00721-010.1016/S0924-0136(03)00721-0 ↗
8. 10.1016/j.ijmecsci.2014.01.01810.1016/j.ijmecsci.2014.01.018 ↗
9. 10.1016/j.matdes.2014.01.07210.1016/j.matdes.2014.01.072 ↗
10. 10.1179/174328405X7163910.1179/174328405X71639 ↗
11. 10.1016/S1003-6326(06)60270-710.1016/S1003-6326(06)60270-7 ↗
12. 10.1016/j.jmatprotec.2006.03.20910.1016/j.jmatprotec.2006.03.209 ↗
13. Qian D. S., and Hua L. ‘Blank design optimisation for T-section profile ring rolling’, Ironmak. Steelmak. 2009, 36, 462–469.10.1179/174328109X443310 ↗
14. 10.1016/j.msea.2009.12.01610.1016/j.msea.2009.12.016 ↗
15. 10.1016/S1003-6326(13)62923-410.1016/S1003-6326(13)62923-4 ↗
16. 10.1016/j.jmatprotec.2010.11.02210.1016/j.jmatprotec.2010.11.022 ↗
17. 10.1016/j.matdes.2010.11.00710.1016/j.matdes.2010.11.007 ↗
18. 10.1007/s11771-014-1909-410.1007/s11771-014-1909-4 ↗
19. 10.1016/j.jmatprotec.2007.04.13510.1016/j.jmatprotec.2007.04.135 ↗
20. 10.1007/BF0264511510.1007/BF02645115 ↗
21. 10.1016/S1359-6454(97)00120-110.1016/S1359-6454(97)00120-1 ↗