journal article·2006-09

Microstructure and properties of austempered ductile iron subjected to single and two step processing

E. V. Pereloma, C. S. Anderson

Materials Science and Technology· Volume 22· Issue 9
Publisher page

Abstract

The predicted processing window has been used to select temperature–time parameters for austempering of a 3·39C–2·28Si–0·48Mn–0·13Mo–0·23Cu–0·05Ni–0·034Mg (wt-%) ductile iron. Comparison of a single step austempering with two step high–low temperature regime has been carried out. The results have shown that with increasing austempering temperature from 300 to 380°C, the morphology of ausferritic ferrite changes from lenticular or lath to feathery, accompanied by an increase in the volume fraction of high carbon retained austenite and carbon concentration in it. This microstructural evolution leads to an increase in ductility and impact energy, but a decrease in strength and hardness after high temperature treatment. All samples have satisfied the mechanical properties of ASTM 897M:1990. Two step high–low (380–340°C) temperature austempering produced microsturctures similar to those seen in high temperature single step processes but with significant time savings. The improvement in the mechanical properties was also achieved after 380–340°C two step processing.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metallurgy and Material Forming · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (24)

Show source-provided references
1. Keough J. R. · Foundry Manag. Technol · 1995 · 123 · 28
2. Elliot R. · Heat Treat. Met · 1997 · 3 · 55
3. Ahlstrand V.: in ‘Heavy duty vehicle braking and steering’, Special publication 1307, 13-18; 1997, Warrendale, PA, Society of Automotive Engineers.
4. Yamakawa S., Kobayashi M., Numajiri S., and Nakashima K. ‘Truck and bus transmissions’, Special addition 1309, 17-22; 1997, Warrendale, PA, Society of Automotive Engineers.
5. Kovacs B. V. · AFS Trans · 1994 · 102 · 417
6. ASTM A- 897M: ‘Annual book of ASTM standards’, 03.01, 576; 1992, Philadelphia, PA, ASTM.
7. Moore D. J. · AFS Trans · 1986 · 94 · 255
8. 10.1179/mst.1996.12.8.67910.1179/mst.1996.12.8.679 ↗
9. 10.1179/mst.1996.12.9.78010.1179/mst.1996.12.9.780 ↗
10. 10.1179/mst.1997.13.4.31910.1179/mst.1997.13.4.319 ↗
11. Yazdani S., and Elliott R. ‘Thermomechanical processing and mechanical properties of hypereutectoid steels and irons’, 101-116; 1997, Warrendale, PA, TMS.
12. 10.1179/mst.1992.8.11.98510.1179/mst.1992.8.11.985 ↗
13. Chester N. A. · J. Phys. IV (France) · 1997 · 7 · 4110.1051/jp4:1997506 ↗
14. 10.1179/02670830110150961010.1179/026708301101509610 ↗
15. 10.1179/02670840222500715910.1179/026708402225007159 ↗
16. 10.1179/mst.1997.13.2.11710.1179/mst.1997.13.2.117 ↗
17. 10.1016/S0921-5093(01)01210-210.1016/S0921-5093(01)01210-2 ↗
18. 10.4028/www.scientific.net/MSF.426-432.91310.4028/www.scientific.net/MSF.426-432.913 ↗
19. ASTM E- 8M: ‘Annual book of ASTM standards’, 03.01, 542-566; 1993, Philadelphia, PA, ASTM.
20. ASTM E- 399: ‘Annual book of ASTM standards’, 03.01, 745; 1992, Philadelphia, PA, ASTM.
21. Kovacs B. V. · Modern Cast · 1987 · 6 · 34
22. 10.1179/174328413X1378982429386710.1179/174328413X13789824293867 ↗
23. Cullity B. D. ‘Elements of X-ray diffraction’, 2nd edn, 411-417; 1978, London, Addison-Wesley Series in Metallurgy and Materials, Addison-Wesley Publishing Company.
24. 10.1016/S1044-5803(98)00005-910.1016/S1044-5803(98)00005-9 ↗