SCC behaviours of austenitic stainless steel Z3CN20-09M in high temperature water
Source abstract
Abstract
Stress corrosion cracking (SCC) behaviours of Z3CN20-09M stainless steel in high temperature water containing Cl−were studied. The results indicated that SCC sensitivity was inconsistent with test temperature. The minimum and maximum of SCC sensitivity occurred at 320 and 290°C respectively, and SCC sensitivity at 250°C fell between them. SCC crack initiated preferentially at bottom of corrosion pit or along phase boundary between austenite and ferrite, and its propagation depended on relative orientation to the phase boundary. SCC crack parallel to the phase boundary propagated along the phase boundary, while that perpendicular to the phase boundary was hindered to propagate.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
National Center for Materials Service Safety, University of Science and Technology Beijing, Beijing 100083, China
Frontier Research Initiative, New Industry Creation Hatchery Center, Tohoku University, 6-6-01 Aoba, Aramaki, Aoba-ku, Sendai 980-8579, Japan
References (34)
Show source-provided references
1. 10.1179/1743278212Y.000000004910.1179/1743278212Y.0000000049 ↗
2. 10.1179/1743278212Y.000000005710.1179/1743278212Y.0000000057 ↗
3. 10.1179/1743278210Y.000000000410.1179/1743278210Y.0000000004 ↗
4. 10.1016/0308-0161(94)00136-710.1016/0308-0161(94)00136-7 ↗
5. Scott PM and Benhamou C: ‘An overview of recent observation and interpretation of IGSCC in nickel base alloys in PWR primary water’, Proc. 10th Int. Symp. on ‘Environmental degradation materials nuclear power systems–water reactors’, NACE, 2001.
6. 10.5006/1.331610410.5006/1.3316104 ↗
7. 10.1016/0029-5493(71)90010-010.1016/0029-5493(71)90010-0 ↗
8. 10.1016/0010-938X(85)90002-210.1016/0010-938X(85)90002-2 ↗
9. Chopra OK and Park HB: ‘Mechanism of fatigue crack initiation in light water reactor coolant environments’, Proc. Int. Conf. on ‘Fatigue of reactor components’, Electric Power Research Institute, 2000.
10. 10.1016/0010-938X(85)90006-X10.1016/0010-938X(85)90006-X ↗
11. Arioka K: ‘Effect of temperature, hydrogen, and boric acid concentration on IGSCC susceptibility of annealed 316 stainless steel’, Proc. Int. Symp. Fontevraud 5, French Nuclear Society, 2002.
12. Arioka K, Kaneshima K and Yamada T: ‘Influence of hydrogen, boric acid, and grain boundary carbide on IGSCC behaviors of SUS316 under hydrogenated PWR primary water’, Proc. 11th Int. Symp. on ‘Environmental degradation of materials in nuclear power systems—water reactors’, American Nuclear Society, 2003.
13. Andresen PL and Angeliu TM: ‘Effect of martensite and hydrogen on SCC of stainless steels and Alloy 600’, Proc. CORROSION/2001, NACE, 2001.10.5006/C2001-01228 ↗
14. 10.5006/1.327832910.5006/1.3278329 ↗
15. Andresen PL and Angeliu TM: ‘Effect of deformation on SCC of unsensitized stainless steel’, Proc. CORROSION/2000, NACE, 2000.10.5006/C2000-00203 ↗
16. 10.5006/1.327831710.5006/1.3278317 ↗
17. Agrawal AK, Welch GA, Begley JA and Staehle RW: ‘SCC of sensitized and quench-annealed type 304 stainless steel in high-purity water’, Proc. CORROSION/1978, NACE, 1978.10.5006/C1978-78187 ↗
18. Arioka K, Hourai M, Okamoto S and Onimura K: ‘The effect of boric acid, solution temperature, and sensitization on SCC behavior under elevated temperature water’, in: CORROSION/83, NACE, 1983.10.5006/C1983-83135 ↗
19. 10.5006/1.358495010.5006/1.3584950 ↗
20. 10.5006/1.357782810.5006/1.3577828 ↗
21. 10.1179/mst.1992.8.8.68510.1179/mst.1992.8.8.685 ↗
22. 10.1179/02670830112500032010.1179/026708301125000320 ↗
23. 10.1179/1743284713Y.000000036510.1179/1743284713Y.0000000365 ↗
24. 10.1016/j.nucengdes.2009.06.00910.1016/j.nucengdes.2009.06.009 ↗
25. 10.1016/j.nucengdes.2010.04.04410.1016/j.nucengdes.2010.04.044 ↗
26. 10.1016/j.engfailanal.2010.09.02210.1016/j.engfailanal.2010.09.022 ↗
27. 10.1016/j.msea.2012.04.10510.1016/j.msea.2012.04.105 ↗
28. 10.1002/9781118787618.ch2410.1002/9781118787618.ch24 ↗
29. 10.1002/9781118787618.ch2210.1002/9781118787618.ch22 ↗
30. Vaillant F, Amzallag C and Champredonde J: ‘Crack growth rate measurements of Alloy 600 vessel head penetrations’, Proc. 8th Int. Symp. on ‘Environmental degradation of materials in nuclear power systems – water reactors’, American Nuclear Society, 1997.
31. 10.5006/1.329356210.5006/1.3293562 ↗
32. 10.1016/0010-938X(87)90068-010.1016/0010-938X(87)90068-0 ↗
33. 10.1016/0010-938X(91)90125-910.1016/0010-938X(91)90125-9 ↗
34. 10.1016/0010-938X(86)90024-710.1016/0010-938X(86)90024-7 ↗