Semisolid deformation of aluminium alloy 356 with non-dendritic structure
Source abstract
Abstract
During semisolid deformation of aluminium alloy 356, as the deformation strain increases, the deformation stress first increases to reach a peak value, then decreases to a minimum value, after which the stress increases towards the end of the deformation. The deformation stress increases as the deformation rate increases at the beginning of the deformation. The increase in the stress towards the end of the deformation is larger as the deformation rate decreases. The difference between the first peak stress and the minimum stress increases as the deformation rate increases. The stress decreases as the deformation temperature increases. The difference between the first peak stress and the minimum stress decreases as the segregation rate increases. The increase in the stress towards the end of the deformation is larger as the segregation rate increases. The degree of segregation is the highest at the middle deformation temperature.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Metallurgy and Material Forming · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. 10.1007/BF0264258010.1007/BF02642580 ↗
2. 10.1007/BF0266109010.1007/BF02661090 ↗
3. BROWN S. B. · Adv. Mater. Process · 1993 · 143 · 36
4. 10.1007/BF0098076310.1007/BF00980763 ↗
5. 10.1007/BF0265511210.1007/BF02655112 ↗
6. 10.1007/BF0264783710.1007/BF02647837 ↗
7. 10.1016/0956-716X(94)90305-010.1016/0956-716X(94)90305-0 ↗
8. 10.1007/BF0035590110.1007/BF00355901 ↗
9. 10.1016/0025-5416(84)90063-610.1016/0025-5416(84)90063-6 ↗
10. 10.1243/PIME_PROC_1993_207_055_0210.1243/PIME_PROC_1993_207_055_02 ↗
11. 10.1179/03071698480327458510.1179/030716984803274585 ↗
12. 10.1016/0020-7403(85)90009-810.1016/0020-7403(85)90009-8 ↗
13. 10.1007/BF0265867210.1007/BF02658672 ↗
14. lotion M. · J. Mater. Shaping Technol., · 1990 · 8 · 3910.1007/BF02834792 ↗
15. 10.1007/BF0266107610.1007/BF02661076 ↗
16. 10.1007/BF0036070310.1007/BF00360703 ↗
17. 10.1016/S1359-6454(96)00312-610.1016/S1359-6454(96)00312-6 ↗
18. S. WASCO, A. ORRIS, P. RAGHUPATHI, and S. L. SEMIATIN: in ‘Forging Handbook’, 156–170; 1985, Metals Park, OH, American Society for Metals.
19. T. H. COURTNEY: ‘Mechanical behavior of materials’, 16–22; 1990, New York, NY, McGraw-Hill.