journal article·2015-03

Characteristics of defect bands and their formation mechanisms in A356 wheel fabricated by horizontal squeeze casting

X. S. Huang, L. J. He, G. B. Mi, P. J. Li

Materials Science and Technology· Volume 31· Issue 4
Publisher page

Abstract

Based on the opinion that a decreasing solid fraction gradient in the cross-section develops during the intensification stage, the shear stress in the solidifying alloy was analysed, and a mechanism for dilatant band formation was discussed. That is, when the shear stress at one position of the stable grain network reaches a critical value, the network collapses and the band forms. The characteristics of defect bands at different locations of an A356 wheel fabricated by horizontal squeeze casting were then studied. Three types of defect bands, i.e. skin related band, dilatant band and separate band, were observed. Combining the process and conditions of defect band formation, several types of defect bands in the casting were discussed. Furthermore, the influence of the structural characteristics of castings on the defect bands, including thickness, geometry and location, was summarised.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Metallurgy and Material Forming · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical Engineering, Tsinghua University, Beijing 100084, China

National Centre of Novel Materials for International Research, Tsinghua University, Beijing 100084, China

References (29)

Show source-provided references
1. 10.1016/S0924-0136(00)00545-810.1016/S0924-0136(00)00545-8 ↗
2. 10.1016/j.matdes.2010.04.00510.1016/j.matdes.2010.04.005 ↗
3. 10.1179/174313309X44930910.1179/174313309X449309 ↗
4. 10.1007/s11661-007-9243-110.1007/s11661-007-9243-1 ↗
5. 10.1007/s11661-010-0222-610.1007/s11661-010-0222-6 ↗
6. 10.4028/www.scientific.net/MSF.419-422.14710.4028/www.scientific.net/MSF.419-422.147 ↗
7. 10.1179/13640460522502321610.1179/136404605225023216 ↗
8. 10.1038/nature0542610.1038/nature05426 ↗
9. 10.1016/S1359-6454(98)00342-510.1016/S1359-6454(98)00342-5 ↗
10. 10.1007/s11661-004-0236-z10.1007/s11661-004-0236-z ↗
11. 10.1016/j.msea.2005.08.19410.1016/j.msea.2005.08.194 ↗
12. Kotadia HR: ‘Solidification behaviour of Al–Sn–Cu immiscible alloys and Al–Si cast alloys processed under intensive shearing’, PhD thesis, Brunel University, Uxbridge, UK, 2010, 82–91.
13. 10.1016/S1003-6326(09)60369-110.1016/S1003-6326(09)60369-1 ↗
14. 10.1016/j.actamat.2008.03.02010.1016/j.actamat.2008.03.020 ↗
15. 10.1140/epje/i2010-10660-910.1140/epje/i2010-10660-9 ↗
16. Munson BR, Young DF, Okiishi TH and Huebsch WW: ‘Fundamentals of fluid mechanics’, 6th edn, Chap. 8, ‘Viscous flow in pipes’, 390–394; 2009, Hoboken, NJ, John Wiley & Sons, Inc.
17. 10.1103/PhysRevE.75.05130610.1103/PhysRevE.75.051306 ↗
18. 10.1209/0295-5075/102/4800210.1209/0295-5075/102/48002 ↗
19. 10.1016/j.jnnfm.2009.12.00110.1016/j.jnnfm.2009.12.001 ↗
20. 10.2320/matertrans.M201303210.2320/matertrans.M2013032 ↗
21. 10.1115/1.290192810.1115/1.2901928 ↗
22. 10.1179/136404610X1269353727025310.1179/136404610X12693537270253 ↗
23. Ashiri R · Mater. Sci. Technol.
24. 10.1016/S0921-5093(02)00747-510.1016/S0921-5093(02)00747-5 ↗
25. 10.1007/s11661-005-1011-510.1007/s11661-005-1011-5 ↗
26. 10.1016/S1471-5317(01)00002-510.1016/S1471-5317(01)00002-5 ↗
27. 10.1007/s11661-009-9841-110.1007/s11661-009-9841-1 ↗
28. 10.1007/s11661-007-9169-710.1007/s11661-007-9169-7 ↗
29. 10.1016/j.scriptamat.2005.01.00710.1016/j.scriptamat.2005.01.007 ↗